Microwave dielectric properties of low-fired Li2SnO3 ceramics co-doped with MgO–LiF

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

2
11
0

Year Published

2017
2017
2023
2023

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 25 publications
(13 citation statements)
references
References 27 publications
2
11
0
Order By: Relevance
“…With addition of 1/7 mol Mg contents, a secondary phase of Li 2 Mg 3 SnO 6 (JCPDS# 39‐0932) was detected accompanied by a reduction of Li 2 SnO 3 phase, and the intensity of (002) peak sharply decreased. This phenomena was in agreement with Keulen et al's report of Li/Sn/Mg catalysts and Fu et al's investigation of Li 2 SnO 3 co‐doped with MgO and LiF, which indicated the following chemical reaction happened:Li2SnnormalO3false(monoclinic(C2/c)false)+3MgOfalse(cubic(Fm3¯m)false)Li2Mg3SnO6false(cubic3(Fm3¯m)false)XRD results demonstrated the existence of Li 2 Mg 3 SnO 6 by the presence of 2θ = 42.57° characteristic peak and will be further evidenced by refinement of XRD and EDX analysis later. Meanwhile, our XRD results were different to the Castellanos's study of phase diagram for the join Li 2 SnO 3 –MgO system where only Li 4 MgSn 2 O 7 or Li 2 SnO 3 existed in the range of 0 < x ≤ 1/7.…”
Section: Resultssupporting
confidence: 91%
See 4 more Smart Citations
“…With addition of 1/7 mol Mg contents, a secondary phase of Li 2 Mg 3 SnO 6 (JCPDS# 39‐0932) was detected accompanied by a reduction of Li 2 SnO 3 phase, and the intensity of (002) peak sharply decreased. This phenomena was in agreement with Keulen et al's report of Li/Sn/Mg catalysts and Fu et al's investigation of Li 2 SnO 3 co‐doped with MgO and LiF, which indicated the following chemical reaction happened:Li2SnnormalO3false(monoclinic(C2/c)false)+3MgOfalse(cubic(Fm3¯m)false)Li2Mg3SnO6false(cubic3(Fm3¯m)false)XRD results demonstrated the existence of Li 2 Mg 3 SnO 6 by the presence of 2θ = 42.57° characteristic peak and will be further evidenced by refinement of XRD and EDX analysis later. Meanwhile, our XRD results were different to the Castellanos's study of phase diagram for the join Li 2 SnO 3 –MgO system where only Li 4 MgSn 2 O 7 or Li 2 SnO 3 existed in the range of 0 < x ≤ 1/7.…”
Section: Resultssupporting
confidence: 91%
“…It was noticeable that a weak vibration mode at around 643 cm −1 was detected at x = 1/7 for the first time. And the appearance of the new mode for XRD was correlated to the single Li/Sn/Mg–O vibration mode in Li 2 Mg 3 SnO 6 phase . Although the Li 4 MgSn 2 O 7 phase was observed in XRD pattern for x = 1/5 and 1/4, no special Raman peaks could be detected and some peaks at around 261 and 317 cm −1 even disappeared.…”
Section: Resultsmentioning
confidence: 92%
See 3 more Smart Citations