2009
DOI: 10.1295/polymj.pj2009079
|View full text |Cite
|
Sign up to set email alerts
|

Microwave-assisted Ring-Opening Polymerization of ε-Caprolactone in Presence of Hydrogen Phosphonates

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
5
0
1

Year Published

2011
2011
2023
2023

Publication Types

Select...
4
4
1

Relationship

1
8

Authors

Journals

citations
Cited by 11 publications
(7 citation statements)
references
References 39 publications
(34 reference statements)
0
5
0
1
Order By: Relevance
“…The effects of the presence of diisopropyl hydrogen phosphonate (2.9%) on the microwave assisted synthesis of PCL was examined, concluding that the ROP was initiated by traces of water but could be catalyzed by the oligo(ε-caprolactone)-substituted hydrogen phosphonate resulting from transesterification reactions. A polymer with molecular weight of 8,100 g/mol was obtained in 100 min at 510 W of irradiation power (Tan et al, 2009). …”
Section: Poly(ε-caprolactone)mentioning
confidence: 99%
“…The effects of the presence of diisopropyl hydrogen phosphonate (2.9%) on the microwave assisted synthesis of PCL was examined, concluding that the ROP was initiated by traces of water but could be catalyzed by the oligo(ε-caprolactone)-substituted hydrogen phosphonate resulting from transesterification reactions. A polymer with molecular weight of 8,100 g/mol was obtained in 100 min at 510 W of irradiation power (Tan et al, 2009). …”
Section: Poly(ε-caprolactone)mentioning
confidence: 99%
“…(2.3–2.5 ppm), and CH 3 (1.2–1.5 ppm) generated from the polymerization of EDA . Moreover, the signals belonged to CH 2 CH 2 CH 2 CH 2 CH 2 (1.4–1.6 ppm), and CH 2 CH 2 CH 2 CH 2 CH 2 (1.1–1.2 ppm) refer to PCL segments . Figure e is the 13 C NMR spectrum of the obtained polymer, the peaks at δ 173.2 and 157.8 ppm can be referred to carbonyl groups.…”
Section: Resultsmentioning
confidence: 93%
“…Poly(ε-caprolactone) (PCL) is one of the most common industrial biodegradable materials for bio- and medical packaging applications. Ring opening polymerization (ROP) of ε-caprolactone(ε-CL) to obtain PCL requires over 24 h when conventional heating is used [99]. Liao et al obtained PCL in just 30 min by performing ROP with ZnO as a catalyst and under the presence of [Bmim][BF 4 ].…”
Section: Polymers Preparationmentioning