Microstructure, mechanical properties and stress corrosion cracking of Al–Zn–Mg–Zr alloy sheet with trace amount of Sc

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
12
0

Year Published

2016
2016
2023
2023

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 48 publications
(12 citation statements)
references
References 55 publications
0
12
0
Order By: Relevance
“…It has also been found that there are precipitation-free zones (PFZ) in the vicinity of grain boundaries ( Figure 4 c). This microstructure is characteristic for Al–Zn–Mg alloys subjected to heat treatment [ 25 , 26 , 27 ]. Deschamps et al [ 9 ] found that the critical factor shaping the microstructure of Al–Zn–Mg–Zr alloys, in addition to degradation and morphology of the Al 3 Zr phase, is also the volume fraction of GP zones, because they are privileged nucleation areas of the η’ phase.…”
Section: Resultsmentioning
confidence: 99%
See 2 more Smart Citations
“…It has also been found that there are precipitation-free zones (PFZ) in the vicinity of grain boundaries ( Figure 4 c). This microstructure is characteristic for Al–Zn–Mg alloys subjected to heat treatment [ 25 , 26 , 27 ]. Deschamps et al [ 9 ] found that the critical factor shaping the microstructure of Al–Zn–Mg–Zr alloys, in addition to degradation and morphology of the Al 3 Zr phase, is also the volume fraction of GP zones, because they are privileged nucleation areas of the η’ phase.…”
Section: Resultsmentioning
confidence: 99%
“…This results in growth and coagulation of precipitates at the boundaries and their distribution in large intervals between them. The precipitation-free zone is also reduced [ 25 , 26 , 27 , 35 ].…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…It was confirmed that Sc addition can significantly improve strength and SCC resistance of 7xxx series alloys [16][17][18][19][20][21][22]. For example, Kannan et al [17] reported the addition of Sc into 7010 Al alloys could introduce a large number of nanosized Al 3 (Sc, Zr) phases to strengthen the alloy and inhibit recrystallization, at the same time, SCC susceptibility of the alloy in neutral 3.5% NaCl solution was reduced.…”
Section: Introductionmentioning
confidence: 91%
“…AA7075. Applying intermediate artificial ageing followed by paint bake and (or) curing thermal cycles would significantly reduce the time required for artificial aging, from 48 hours to less than 2 hours, which could save energy significantly and enhance productivity [15][16][17].…”
Section: Introductionmentioning
confidence: 99%