2017
DOI: 10.1016/s1003-6326(17)60191-2
|View full text |Cite
|
Sign up to set email alerts
|

Microstructure characterization of Al-cladded Al–Zn–Mg–Cu sheet in different hot deformation conditions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2018
2018
2022
2022

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 10 publications
(2 citation statements)
references
References 22 publications
0
2
0
Order By: Relevance
“…As for pre-aged samples, the yield strength increment due to dislocations strengthening contribution and the dislocation density are listed in table 4. It shows that the contribution difference of dislocation strengthening to the yield strength between the samples in pre-aged (along axial, along hoop and along radial) is negligible basically, so the yeild strength anisotropy caused by dislocation strengthening can be ignored after pre-aging stage.…”
Section: Dislocation Strengtheningmentioning
confidence: 99%
See 1 more Smart Citation
“…As for pre-aged samples, the yield strength increment due to dislocations strengthening contribution and the dislocation density are listed in table 4. It shows that the contribution difference of dislocation strengthening to the yield strength between the samples in pre-aged (along axial, along hoop and along radial) is negligible basically, so the yeild strength anisotropy caused by dislocation strengthening can be ignored after pre-aging stage.…”
Section: Dislocation Strengtheningmentioning
confidence: 99%
“…7xxx series aluminum alloys are widely used in aviation field because of their low density, ultra-high strength and high toughness [1][2][3][4][5]. The mechanical properties of this kind of alloys mainly depend on the precipitation characteristics during aging.…”
Section: Introductionmentioning
confidence: 99%