“…Flexural strength of cast samples was determined by performing 3-point bend testing using a mechanical testing stage (SEMtester 1000, MTI Instruments, Inc., Albany, NY, USA) as shown in Fig. 3.4 [92] . Due to the high flexibility of the dip coated samples, they 2 contact locations and applying a force at a third central contact location (Fig.…”