Microstructure and mechanical properties of rolled sheets of Mg–Gd–Y–Zn–Zr alloy: As-cast versus as-homogenized

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
14
0

Year Published

2013
2013
2022
2022

Publication Types

Select...
8
1

Relationship

1
8

Authors

Journals

citations
Cited by 40 publications
(14 citation statements)
references
References 24 publications
0
14
0
Order By: Relevance
“…Xu et al [94] reported that the as cast Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr alloy consisted of α-Mg grains surrounded by Mg3(Gd,Y) eutectic compounds while the as-homogenized alloy consisted of 18R and 14 H type LPSO phases which was attributed to the higher strength of as-homogenized alloy. The same authors reported in [95] that the Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr alloy exhibited better properties when it is rolled with 96% reduction.…”
Section: Mg-zn-re Higher Alloy Systemsmentioning
confidence: 99%
“…Xu et al [94] reported that the as cast Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr alloy consisted of α-Mg grains surrounded by Mg3(Gd,Y) eutectic compounds while the as-homogenized alloy consisted of 18R and 14 H type LPSO phases which was attributed to the higher strength of as-homogenized alloy. The same authors reported in [95] that the Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr alloy exhibited better properties when it is rolled with 96% reduction.…”
Section: Mg-zn-re Higher Alloy Systemsmentioning
confidence: 99%
“…9 shows the nominal tensile stress-strain curves of homogenized samples followed by different cooling rates. The corresponding tensile yield strength (TYS), ultimate tensile strength (UTS) and elongation to failure are summarized in Table 1; the tensile properties of the as-cast alloy [24] is also given in Table 1 for comparison. The as-cast alloy exhibits poor tensile properties due to the network shaped eutectic phases.…”
Section: Microstructure Of the Homogenized Alloy Followed By Cooling mentioning
confidence: 99%
“…The micro-crack generated easily from these coarse particles, and as a result of high volume of precipitates, too many micro-cracks initiated from these precipitates and connected to each other till the formation of the macro-cleavage [13]. It is the residual stress and high volume of precipitates deteriorating the ductility of the samples forged and compressed at lower temperature [14].…”
Section: Mechanical Propertiesmentioning
confidence: 99%