2015
DOI: 10.1016/j.ceramint.2014.09.115
|View full text |Cite
|
Sign up to set email alerts
|

Microstructure and mechanical properties of B4C densified by spark plasma sintering with Si as a sintering aid

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
10
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 44 publications
(10 citation statements)
references
References 14 publications
(18 reference statements)
0
10
0
Order By: Relevance
“…All hot-pressed B 4 C-ZrB 2 samples achieve nearly full densification. Owing to its strong covalent bonding and low self-diffusion coefficient, monolithic B 4 C ceramic is always hard to achieve full densification and is reported to be densified above 2100°C [6,7]. The introduction of appropriate second phase particle is proved to be an efficient method to improve the sinterability.…”
Section: Resultsmentioning
confidence: 98%
See 2 more Smart Citations
“…All hot-pressed B 4 C-ZrB 2 samples achieve nearly full densification. Owing to its strong covalent bonding and low self-diffusion coefficient, monolithic B 4 C ceramic is always hard to achieve full densification and is reported to be densified above 2100°C [6,7]. The introduction of appropriate second phase particle is proved to be an efficient method to improve the sinterability.…”
Section: Resultsmentioning
confidence: 98%
“…Despite of attractive application properties of B 4 C, its applicability mainly limits to its poor sinterability [6,7] and low fracture toughness [8,9]. The poor sinterability of B 4 C is mainly due to the strong covalent bonding and low self-diffusion coefficient.…”
Section: Introductionmentioning
confidence: 98%
See 1 more Smart Citation
“…As compared in Table , this reactive sintering with in situ carbothermal reduction of B 4 C at ~1250 to 1400°C without pressurization resulted in low relative densities (57.7%‐62.8%), but these densities are comparable with those of pressureless sintering conducted at much higher temperatures (>2000°C) when no additives were introduced. While the papers reviewed in Table are limited to densification of monolithic B 4 C powders, densification with additives has been studied to increase densification: hydrogen and carbon to reduce oxygen or B 2 O 3 , and liquid phases (Si, Cr 3 C 2 , and Al) to enhance densification at lower temperatures.…”
Section: Resultsmentioning
confidence: 99%
“…However, low strength of B 4 C is the major application impediment [4][5][6]. Moreover, due to its very strong covalent bonds, high resistance to grain interface sliding and lack of plasticity, densification of B 4 C is extremely difficult and costly [7][8][9].…”