Microstructure and Mechanical Properties of Inconel 718 Produced by SLM and Subsequent Heat Treatment

Abstract: The article presents results of selective laser melting of Inconel 718 superalloy. It was studied phase microstructure of the material obtained by selective laser melting and also the material after heat treatment. The phase composition of the initial powder material, the specimens after selective laser melting before and after heat treatment was studied. The effect of heat treatment on microstructure and mechanical properties of the specimens was shown. It was studied the mechanical behavior of the manufactur… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
21
0
8

Year Published

2016
2016
2022
2022

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 71 publications
(30 citation statements)
references
References 6 publications
1
21
0
8
Order By: Relevance
“…As that for titanium alloys, employing SLM or EBM to manufacture Ni-base superalloys would depend on the specific case or application, since each process has its pros and cons. So far, the Ni-base superalloys applied to SLM are mainly the weldable ones, i.e., IN718 [113,[160][161][162][163][164][165][166][167], IN625 [79,80,168,169], Hastelloy X [170][171][172][173][174], Nimonic 263 [110], which have low additions of both Ti and Al and are less susceptible to strain age cracking. Expansion to the less-weldable Ni-base superalloys has also been attempted, such as IN939 [175], IN100 [176], IN738LC [177][178][179][180][181], CM247LC [114,[182][183][184] and Rene 142 [81].…”
Section: Materials Manufactured With Slmmentioning
confidence: 99%
“…As that for titanium alloys, employing SLM or EBM to manufacture Ni-base superalloys would depend on the specific case or application, since each process has its pros and cons. So far, the Ni-base superalloys applied to SLM are mainly the weldable ones, i.e., IN718 [113,[160][161][162][163][164][165][166][167], IN625 [79,80,168,169], Hastelloy X [170][171][172][173][174], Nimonic 263 [110], which have low additions of both Ti and Al and are less susceptible to strain age cracking. Expansion to the less-weldable Ni-base superalloys has also been attempted, such as IN939 [175], IN100 [176], IN738LC [177][178][179][180][181], CM247LC [114,[182][183][184] and Rene 142 [81].…”
Section: Materials Manufactured With Slmmentioning
confidence: 99%
“…При получении образцов исполь-зованы режимы, обеспечивающие наибольшую плотность, как было показано в предыдущих на-ших работах [11,22]. Принципиальная схема про-цесса СЛП представлена на рис.…”
Section: методика исследований и оборудованиеunclassified
“…Исследования микроструктуры полученных по технологии СЛП образцов, представленные в работах [2][3][4][5][6][7][8][9][10][11] …”
Section: Introductionunclassified
See 2 more Smart Citations