2022
DOI: 10.1016/j.ceramint.2022.02.070
|View full text |Cite
|
Sign up to set email alerts
|

Microstructure and mechanical properties of hot-pressed SiC nanofiber reinforced SiC composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
5
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 7 publications
(5 citation statements)
references
References 26 publications
0
5
0
Order By: Relevance
“…SiC nw pull‐out and bridging indicates the obtained suitable bonding strength between the matrix and the reinforcement. Moreover, the pull‐out length of the SiC nw in this experiment is larger than that of the SiC nw /SiC CMC without interface coating 22 . It can be attributed to the weak interface provided by the BN interface for the composite, thereby promoting the fiber pull‐out and debonding.…”
Section: Resultsmentioning
confidence: 74%
See 3 more Smart Citations
“…SiC nw pull‐out and bridging indicates the obtained suitable bonding strength between the matrix and the reinforcement. Moreover, the pull‐out length of the SiC nw in this experiment is larger than that of the SiC nw /SiC CMC without interface coating 22 . It can be attributed to the weak interface provided by the BN interface for the composite, thereby promoting the fiber pull‐out and debonding.…”
Section: Resultsmentioning
confidence: 74%
“…The density of the composites was measured using the Archimedes method, and their relative densities were calculated by employing the compound principle. The three‐point flexural test and the single edge‐notched beam test were carried out to study the mechanical properties of the SiC nw /SiC CMC 22 …”
Section: Methodsmentioning
confidence: 99%
See 2 more Smart Citations
“…SiCnws have the characteristics of a high strength and hardness, which are inherited from the SiC ceramic, as well as a good toughness and elasticity, which are typical of nanomaterials [26,27]. Recently, SiCnws have already been utilized in ceramic matrices such as SiC and Al2O3, as well as in ceramic matrix composites like carbon fiber/lithium aluminosilicate, demonstrating outstanding strengthening and toughening effects [28][29][30]. SiCnws could potentially serve as a highly efficacious reinforcing agent for BSAS ceramic.…”
Section: J U S T a C C E P T E Dmentioning
confidence: 99%