Ethylene-propylene-diene terpolymer rubberlnatural rubber blends (EPDM/NR) in different proportions (100 : 0. 75 : 25, 50 : 50. 25 : 75, and 0 : 100) reinforced with 20 phr semireinforcing furnace carbon black have been studied. The permittivity E' and dielectric loss d' for these samples were determined in the frequency range 10'-10' Hz. Also, their physico-mechanical properties were investigated.The EPDM/NR blend (75 : 25) possessed the best mechanical properties and stability against aging. Thus, it was chosen to explore the effect of adding carbon black in different quantities up to 50 phr on its electrical and mechanical properties. Three different types of carbon black. namely high-abrasion furnace black, fast-extrusion furnace black, and medium thermal black, were used. At a certain concentration of carbon black, referred to as the threshold percolation concentration, an abrupt increase in E' and E", which depends on its type, was detected. This could be attributed to some sort of interaction between the blend and the carbon black at higher concentrations.