Micro-mechanisms of a laminated packaging material during fracture

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

2
26
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
6
1

Relationship

1
6

Authors

Journals

citations
Cited by 24 publications
(28 citation statements)
references
References 25 publications
2
26
0
Order By: Relevance
“…This phenomenon has been interpreted at the light of brittle or quasi-brittle fracture models in [2][3][4][5], consistently with the smaller rupture strain and meaningful reduction of toughness exhibited by free-standing thin metal foils compared to the corresponding bulk materials [6,7]. However, fractographical examinations reported in [8] suggest that the material separation may be rather produced by necking, in other words, by a typical elastic-plastic phenomenon.…”
Section: Figure 1 Typical Composition and Functionality Of Beverage mentioning
confidence: 81%
See 2 more Smart Citations
“…This phenomenon has been interpreted at the light of brittle or quasi-brittle fracture models in [2][3][4][5], consistently with the smaller rupture strain and meaningful reduction of toughness exhibited by free-standing thin metal foils compared to the corresponding bulk materials [6,7]. However, fractographical examinations reported in [8] suggest that the material separation may be rather produced by necking, in other words, by a typical elastic-plastic phenomenon.…”
Section: Figure 1 Typical Composition and Functionality Of Beverage mentioning
confidence: 81%
“…Strain localization can be observed also in polyethylene but at much larger elongation values. The graphs in Figure 9b concern the simulation of uniaxial tensile tests performed on plain or notched samples similar to those investigated in [5]. The presence of a centered cut is considered in this case, with crack length equal to about 15% and 50% of the specimen width.…”
Section: Modeling Issuesmentioning
confidence: 99%
See 1 more Smart Citation
“…On the other side, wrinkling phenomena are frequently observed in wide samples and affect the interpretation of the experimental output [10][11][12][13]. These disturbances can be detected by three-dimensional digital correlation techniques [14,15] and potentially reproduced by finite element analysis.…”
Section: Introductionmentioning
confidence: 99%
“…However, these geometries do not permit to calibrate the fracture properties since failure is provoked by an almost instantaneous material separation. Different aspect ratios and pre-notched material samples have been therefore considered in order to follow the fracture evolution and the relevant crack propagation processes [10,11].…”
Section: Introductionmentioning