Mechanical Property Evaluation of Permanent-Mould Cast AM-SC1™ Mg-Alloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2009
2009
2018
2018

Publication Types

Select...
1
1

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(2 citation statements)
references
References 14 publications
0
2
0
Order By: Relevance
“…The sample geometries and the test methods have been described elsewhere [14]. The constant load creep tests in tension were carried out in silicone oil baths, with temperature control better than ±1 K. Three test temperatures were used (423 K, 450 K and 473 K) with several loads applied at each temperature, up to a maximum of 100 MPa.…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…The sample geometries and the test methods have been described elsewhere [14]. The constant load creep tests in tension were carried out in silicone oil baths, with temperature control better than ±1 K. Three test temperatures were used (423 K, 450 K and 473 K) with several loads applied at each temperature, up to a maximum of 100 MPa.…”
Section: Methodsmentioning
confidence: 99%
“…The properties of this alloy for T6 heat treated sand-castings have been described in [13] and for T6 heat treated permanent mould castings in [14]. The alloy is based on the Mg-RE system, and contains additions of Zr for grain refinement purposes.…”
Section: Introductionmentioning
confidence: 99%