Mechanical property and gas filtration behavior of porous reaction bonded Si3N4 with monodispersed PMMA as pore former

Abstract: Porous Si 3 N 4 ceramics were prepared by gel casting combined with a reaction bonding route using monodispersed PMMA as the pore former, and Isobam was used as a gel agent. With the PMMA addition varying from 0 to 20 wt.%, the bending strength was degraded from 94.0 to 39.1 MPa owing to the increased porosity and decreased bulk density. The β-Si 3 N 4 prismatic grains and round pores introduced by the monodispersed PMMA micro balls would endow the samples with high strength, and the permeability of the result… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2

Citation Types

0
4
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 10 publications
(4 citation statements)
references
References 58 publications
(83 reference statements)
0
4
0
Order By: Relevance
“…Furthermore, the pore sizes detected by mercury injection were inconsistent with those observed by SEM 27 . This was because the mercury intrusion test can only detect the so‐called pore‐channel or pore‐neck 31 …”
Section: Resultsmentioning
confidence: 94%
See 3 more Smart Citations
“…Furthermore, the pore sizes detected by mercury injection were inconsistent with those observed by SEM 27 . This was because the mercury intrusion test can only detect the so‐called pore‐channel or pore‐neck 31 …”
Section: Resultsmentioning
confidence: 94%
“…Furthermore, the pore sizes detected by mercury injection were inconsistent with those observed by SEM. 27 This was because the mercury intrusion test can only detect the so-called pore-channel or pore-neck 31 Figure 9A shows apparent porosity and bulk density of porous SiC ceramics with different contents of PMMA. It can be seen that with the increase of PMMA content from 0 to 20 wt%, apparent porosity increased from 22.4% to 57.7%, whereas bulk density decreased from 2.18 to 1.29 g/cm 3 .…”
Section: Resultsmentioning
confidence: 99%
See 2 more Smart Citations