Abstract:Mechanical properties of diamond lattice structures based on main parameters and strain rateThe diamond triply periodic minimal surface structure has a high mechanical property-weight ratio. They can be modified by changing their internal parameters or the material. They are generated using the additive manufacturing (AM) that possibilities the use of various materials for generating zones with different mechanical properties or by modifying their internal parameters.However, the effects of internal parameters… Show more
“…The sample had a cubic shape with outer dimensions of 15.5 mm × 14.8 mm × 15.9 mm and a cell size of 3 mm. The average thickness of the lattice struts equalled to 0.7 mm and the sample had a porosity of 84% [29].…”
“…The sample had a cubic shape with outer dimensions of 15.5 mm × 14.8 mm × 15.9 mm and a cell size of 3 mm. The average thickness of the lattice struts equalled to 0.7 mm and the sample had a porosity of 84% [29].…”
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.