2014
DOI: 10.1007/s11661-014-2294-1
|View full text |Cite
|
Sign up to set email alerts
|

Mechanical Properties Anisotropy of Cold-Rolled and Solution-Annealed Ni-Based Hastelloy C-276 Alloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

3
14
0

Year Published

2014
2014
2018
2018

Publication Types

Select...
8

Relationship

2
6

Authors

Journals

citations
Cited by 36 publications
(17 citation statements)
references
References 22 publications
3
14
0
Order By: Relevance
“…Therefore, the larger grain tentatively carries the greater frequencies for grain fragmentation [12]. Orientation of individual crystallites has crucial role because of the orientation of its characteristic slip system with respect to sample loading reference and therefore, slip heterogeneity and consecutive breaking of grain [22,23]. The role of SFE to fragment grains is eventually crucial.…”
Section: Breaking Tendency Of Tempered Lathmentioning
confidence: 99%
“…Therefore, the larger grain tentatively carries the greater frequencies for grain fragmentation [12]. Orientation of individual crystallites has crucial role because of the orientation of its characteristic slip system with respect to sample loading reference and therefore, slip heterogeneity and consecutive breaking of grain [22,23]. The role of SFE to fragment grains is eventually crucial.…”
Section: Breaking Tendency Of Tempered Lathmentioning
confidence: 99%
“…The schematic diagram of the tensile specimens is given elsewhere. [12] Room temperature tensile tests were conducted at a normal strain rate (10 À3 s À1 ) on screw-driven Instron 4507 testing machine (Instron Corporation, Norwood, MA, USA). The strains were measured using an axial type extensometer (model 1267: Instron U.K.), specified for gage length of 10 mm.…”
Section: Mechanical Propertiesmentioning
confidence: 99%
“…[21] On the contrary, Mehta et al have recently shown different mechanisms responsible for two-slope behavior of solid solution strengthened Ni-based Hastelloy C-276 and Ni20Cr-8Fe alloys. [12,22] At low strains, sample display the presence of annealing twins and less strain localization at the grain boundaries. Whereas formation of deformation twins along with high-strain localization within the deformation twins and at the grain boundaries are the key features in high-strain regime samples.…”
Section: Tensile Flow Behaviormentioning
confidence: 99%
“…The hot rolled microstructures further get modified during solution treatment and subsequent aging. Two types of anisotropy namely, in-plane and through-thickness, have been reported in rolled products [21]. The thin sheet products typically display in-plane anisotropy i.e.…”
Section: Introductionmentioning
confidence: 99%