Mechanical fatigue of biodegradable polymers: A study on polylactic acid (PLA), polybutylene succinate (PBS) and polybutylene adipate terephthalate (PBAT)

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
6
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 16 publications
(6 citation statements)
references
References 64 publications
0
6
0
Order By: Relevance
“…PBAT was obtained from Xinjiang Blue Ridge Tunhe Polyester Co., Ltd (grade TH801T, melting at 110–120°C, tensile strength 25 MPa, elongation at break >500%$>500\%$, Mw ≈ 7.5 × 10 4 g mol −1 . [ 66,67 ] The bio‐based ink for spray coating was made up of only the previously mentioned three components through some straightforward steps. First, one weight % PBAT was dissolved in anisole.…”
Section: Methodsmentioning
confidence: 99%
“…PBAT was obtained from Xinjiang Blue Ridge Tunhe Polyester Co., Ltd (grade TH801T, melting at 110–120°C, tensile strength 25 MPa, elongation at break >500%$>500\%$, Mw ≈ 7.5 × 10 4 g mol −1 . [ 66,67 ] The bio‐based ink for spray coating was made up of only the previously mentioned three components through some straightforward steps. First, one weight % PBAT was dissolved in anisole.…”
Section: Methodsmentioning
confidence: 99%
“…From Equation (), the stress response includes linear and nonlinear parts. The linear part can be combined with the strain signal to get the complex modulus: E*goodbreak=I1ε0 Furthermore, the storage ( E' ) and loss ( E" ) moduli can be easily obtained as: Egoodbreak=E*cos()δ1goodbreak−δ1 Egoodbreak=E*sin()δ1goodbreak−δ1 More details on the experimental setup and data analysis can be found elsewhere 36,37 …”
Section: Methodsmentioning
confidence: 99%
“…Furthermore, the storage (E') and loss (E") moduli can be easily obtained as: More details on the experimental setup and data analysis can be found elsewhere. 36,37 DSC was used to evaluate the thermal properties, such as melting and crystallization. A small amount of material (6-14 mg) was placed in an aluminum pan and the samples were heated and cooled at 10 C min À1 between 50 C and 200 C (300 C) in a nitrogen atmosphere.…”
Section: Characterizationmentioning
confidence: 99%
“…Besides being very tough and its high ductility, other advantages of PBAT include easy processability, biodegradability, biocompatibility, and a high production capacity [ 18 ]. Numerous researchers have developed PBS and PBAT blends and have investigated their properties [ 19 , 20 ]. For instance, Costa et al [ 17 ] fabricated PBS and PBAT blends and investigated their properties.…”
Section: Introductionmentioning
confidence: 99%