Abstract: The multifunctional superhydrophobic surfaces incorporated with Fe3O4 exhibit excellent anti-icing and active deicing properties.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
99
0

Year Published

2017
2017
2022
2022

Publication Types

Select...
7
2

Relationship

0
9

Authors

Journals

citations
Cited by 152 publications
(100 citation statements)
references
References 50 publications
1
99
0
Order By: Relevance
“…As shown in Figure a, chemical structures of the pristine MF sponge, Fe 3 O 4 NPs, PDA‐Fe 3 O 4 @MF, MA‐PDMS monomer, and PDMS‐Fe 3 O 4 @MF were confirmed by Fourier transform infrared (FT‐IR) spectra. Compared with the pristine MF sponge, the PDA‐Fe 3 O 4 @MF spectrum exhibited the characteristic signals of Fe‐O stretching (588 cm −1 ), PDA N‐H shearing (1592 cm −1 ), and PDA aromatic ring C–C vibration (1507 cm −1 ), demonstrating the successful codeposition of Fe 3 O 4 NPs and PDA coating. The spectrum of MA‐PDMS monomer displayed strong adsorption bands of Si‐C bond (at 1261 and 802 cm −1 ) and Si‐O‐Si bond (at 1028 and 1089 cm −1 ) .…”
Section: Resultsmentioning
confidence: 99%
“…As shown in Figure a, chemical structures of the pristine MF sponge, Fe 3 O 4 NPs, PDA‐Fe 3 O 4 @MF, MA‐PDMS monomer, and PDMS‐Fe 3 O 4 @MF were confirmed by Fourier transform infrared (FT‐IR) spectra. Compared with the pristine MF sponge, the PDA‐Fe 3 O 4 @MF spectrum exhibited the characteristic signals of Fe‐O stretching (588 cm −1 ), PDA N‐H shearing (1592 cm −1 ), and PDA aromatic ring C–C vibration (1507 cm −1 ), demonstrating the successful codeposition of Fe 3 O 4 NPs and PDA coating. The spectrum of MA‐PDMS monomer displayed strong adsorption bands of Si‐C bond (at 1261 and 802 cm −1 ) and Si‐O‐Si bond (at 1028 and 1089 cm −1 ) .…”
Section: Resultsmentioning
confidence: 99%
“…in ref. , obtained superhydrophobic nanocomposite films with embedded magnetic nanoparticules exhibiting 2878 s FDT at −15 °C. The highest FDT was observed by X. Zhan et al .…”
Section: Introductionmentioning
confidence: 85%
“…Other than that, for containers 8 Research with high brittleness such as the glass bottle, the icing of the inner content can lead to breach or destruction of the container due to the swelling of the icing content. The introduction of ELIS to packaging materials such as glass could reduce the ice accumulation by reducing the pinning spot for ice nucleation [39,40]. The carnauba wax with CO was chosen as a test surface due to better slippery performance of the coating and lower icing point of CO (approximately -20°C).…”
Section: Icing Delay Experimentmentioning
confidence: 99%