Low viscosity dimethacrylate comonomer compositions [Bis-GMA and CH3Bis-GMA] for novel dental composites; analysis of the network by stray-field MRI, solid-state NMR and DSC & FTIR

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

1
47
0
1

Year Published

2005
2005
2022
2022

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 76 publications
(49 citation statements)
references
References 14 publications
1
47
0
1
Order By: Relevance
“…To overcome these unwanted effects studies have been directed toward developing low viscosity, hydroxyl free, more hydrophobic bis-GMA analogs such as the propoxylated bis-GMA (2,2-bis(4-(2-methacryloxyprop-1-oxy)phenyl)propane), as a replacement for TEGDMA in bis-GMA mixtures 7,8 . The properties of bis-GMA copolymers and composites containing CH 3 bis-GMA ( Figure 1) have been evaluated.…”
Section: Introductionmentioning
confidence: 99%
“…To overcome these unwanted effects studies have been directed toward developing low viscosity, hydroxyl free, more hydrophobic bis-GMA analogs such as the propoxylated bis-GMA (2,2-bis(4-(2-methacryloxyprop-1-oxy)phenyl)propane), as a replacement for TEGDMA in bis-GMA mixtures 7,8 . The properties of bis-GMA copolymers and composites containing CH 3 bis-GMA ( Figure 1) have been evaluated.…”
Section: Introductionmentioning
confidence: 99%
“…Stray-Field Magnetic Resonance Imaging (STRAFI-MRI) has proved its reliability in the study of dental materials [14][15][16][17]. A comparative study of three adhesives (Prime&Bond NT, Single Bond and XENO III) by 1 H STRAFI-MRI is presented.…”
Section: Introductionmentioning
confidence: 99%
“…Low correlation may indicate the possibility of high dependence on the amount of each monomer and their combinations. Among the monomers contained in the tested products (basically, Bis-EMA, Bis-GMA, TEGDMA, and UDMA), TEGDMA showed the lowest viscosity (approximately 0.01 Pa•s) and greatest shrinkage due to low molecular weight (286 g/mol) 23) . Also, it showed the highest water sorption due to hydrophilic nature, however, solubility was the lowest among them.…”
Section: Discussionmentioning
confidence: 99%
“…Also, exceptionally high solubility would be related with much release of uncured residual monomers. Low flow rate of GF and GU would be probably due to the high inclusion of UDMA in addition to their high filler content (UDMA has approximately 10 3 times greater viscosity than TEGDMA) 23) . High solubility of GF among the products can be related with the release of fluoride from LaF 3 (lantanoid fluoride).…”
Section: Discussionmentioning
confidence: 99%