Low‐loss planar optical waveguides fabricated from polycarbonate

Abstract: Low‐loss slab waveguides with air as overcladding based on a high glass transition temperature (Tg) polycarbonate were fabricated through spin‐coating. Optical absorption and thermo‐optic coefficient were investigated by spectrum analysis and prism coupler, respectively. Prism‐coupling and charge‐coupled device (CCD) camera imaging method were exploited together to evaluate the overall propagation loss of slab waveguides. The measured results of prism coupler were 0.282 dB/cm at 1310 nm and 0.197 dB/cm at 632.… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
8
0

Year Published

2012
2012
2019
2019

Publication Types

Select...
8

Relationship

2
6

Authors

Journals

citations
Cited by 19 publications
(9 citation statements)
references
References 18 publications
1
8
0
Order By: Relevance
“…Figure 2 shows the Izod impact strength plotted against the PB rubber content for the different PVC/ABS blends prepared at milling temperatures of 165°C and 180°C. The impact strength of blends increased together with the PB rubber content as expected from previous studies [14,17,18]. At low PB rubber contents, all of the notched impact strength of brittle blends occurred in the range of 50-200 J/m, independent of the type of PVC resin used.…”
Section: Effect Of the Pvc Molecular Weightsupporting
confidence: 65%
See 1 more Smart Citation
“…Figure 2 shows the Izod impact strength plotted against the PB rubber content for the different PVC/ABS blends prepared at milling temperatures of 165°C and 180°C. The impact strength of blends increased together with the PB rubber content as expected from previous studies [14,17,18]. At low PB rubber contents, all of the notched impact strength of brittle blends occurred in the range of 50-200 J/m, independent of the type of PVC resin used.…”
Section: Effect Of the Pvc Molecular Weightsupporting
confidence: 65%
“…The SAN copolymer was supplied by Jilin Petrochemical Corp (Jilin City, Jilin Province, China). The preparation of the ABS modifier is described in detail in our previous published article [14]. The average molecular weight (M w ) and the average molecular number (M n ) for the SAN copolymer were 148,000 and 49,400 g/mol, respectively.…”
Section: Methodsmentioning
confidence: 99%
“…Optical polymeric materials permit the mass production of low-cost integrated optical devices and circuits on a planar substrate [7,8]. Polymer-based optical waveguide is the basic light transmission medium for integrated optical device.…”
Section: Introductionmentioning
confidence: 99%
“…First, computer numerical control (CNC) machining was used to manufacture the PC module and spacer. PC was used because it is inexpensive, easily machinable, and has a relatively high tolerance to heat and impact [24]. Second, an etching process was used to fabricate the Yagi antenna and FR4 reflector.…”
Section: Fabrication Of the Proposed Antennamentioning
confidence: 99%