Local electrochemical surface analysis

Abstract: A review of advances in local electrochemical analysis is presented.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
6
0

Year Published

2005
2005
2013
2013

Publication Types

Select...
5

Relationship

1
4

Authors

Journals

citations
Cited by 5 publications
(6 citation statements)
references
References 7 publications
0
6
0
Order By: Relevance
“…A hybrid method was developed in [29] for the local electrochemical analysis of coatings and thin-film structures. It combines different versions of local electrochemical analysis and stripping voltammetry.…”
Section: Electrode Processesmentioning
confidence: 99%
See 4 more Smart Citations
“…A hybrid method was developed in [29] for the local electrochemical analysis of coatings and thin-film structures. It combines different versions of local electrochemical analysis and stripping voltammetry.…”
Section: Electrode Processesmentioning
confidence: 99%
“…The hybrid method of local electrochemical analysis-stripping voltammetry was used for the quantitative estimation of the phase and elemental composition of Sn, Cu, and Zn alloy coatings [29,39] and thermal InSn alloys [40]. Procedures of hybrid local electrochemical analysis were developed for controlling the composition of an alloy surface under corrosive conditions [41][42][43][44][45].…”
Section: Practical Applicationsmentioning
confidence: 99%
See 3 more Smart Citations