2021
DOI: 10.1016/j.matpr.2020.11.450
|View full text |Cite
|
Sign up to set email alerts
|

Liquid state stir cast processing and characteristics study of AZ91D/SiCp composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
13
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 16 publications
(13 citation statements)
references
References 14 publications
0
13
0
Order By: Relevance
“…Based on ASTM A370 standard, 12 the tensile strength of developed AZ91D alloy composite samples was evaluated by Instron make tensiometer. ASTM E-384 standard, 14 the hardness of the composite sample was evaluated by three different indentations in each composite, and an average with 5% permissible error was considered the mean value.…”
Section: Characterization Studymentioning
confidence: 99%
See 3 more Smart Citations
“…Based on ASTM A370 standard, 12 the tensile strength of developed AZ91D alloy composite samples was evaluated by Instron make tensiometer. ASTM E-384 standard, 14 the hardness of the composite sample was evaluated by three different indentations in each composite, and an average with 5% permissible error was considered the mean value.…”
Section: Characterization Studymentioning
confidence: 99%
“…However, the effective stir casting parameters adopted with SF6's inert nature lead to reduced oxidation during the magnesium melt, 12 a uniform stir speed of 400 rpm enhances the distribution of particle in the matrix, 10 and applied vacuum pressure removes the internal stress. 21…”
Section: Void Percentagesmentioning
confidence: 99%
See 2 more Smart Citations
“…Further, the inclusion WC decreased the wear and increased the wear resistance and strength of composite. Chandradass et al (2020) characterized the stir casted AZ91D/SiC composite and resulted that the tensile strength and hardness were improved by 45% and 34% when adding 2 Wt.% and 5 Wt.% SiC respectively with AZ91D. Further, authors reported that the AZ91D/5 Wt.% SiC composite showed the least wear rate of 0.89 mm 3 /Nm and higher coefficient of friction of 0.425.…”
Section: Introductionmentioning
confidence: 98%