2010
DOI: 10.1007/s00170-009-2489-6
|View full text |Cite
|
Sign up to set email alerts
|

Laser cutting of 7050 Al alloy reinforced with Al2O3 and B4C composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
12
0

Year Published

2013
2013
2020
2020

Publication Types

Select...
7
2

Relationship

0
9

Authors

Journals

citations
Cited by 33 publications
(12 citation statements)
references
References 18 publications
0
12
0
Order By: Relevance
“…Finally, the mold was kept inside the furnace until 250 o C furnace temperature and then placed in the open air to complete the cooling. This method was similar to the fabrication route used by previous researchers [6], [19]- [22].…”
Section: A Ball Milling and Pressingmentioning
confidence: 96%
“…Finally, the mold was kept inside the furnace until 250 o C furnace temperature and then placed in the open air to complete the cooling. This method was similar to the fabrication route used by previous researchers [6], [19]- [22].…”
Section: A Ball Milling and Pressingmentioning
confidence: 96%
“…This method is, in fact, the standard procedure to produce Al-based composites [6,[20][21][22][23], where consequently, three different batches of composites with different percentages of B 4 C content were produced (Table 1).…”
Section: Manufacturing the Materialsmentioning
confidence: 99%
“…Following that operation, the materials were placed in an electrical furnace, and the materials were sintered at 540°C in a liquid phase for half an hour. This production technique was similar to the fabrication route used by previous Al, c Zn, d Cu researchers [10][11][12]. The microstructure of composite was shown in Fig.…”
Section: Production Of the Composite Materialsmentioning
confidence: 99%