2017
DOI: 10.1039/c7tc02206a
|View full text |Cite
|
Sign up to set email alerts
|

Large tunable luminescence by Mn(ii) aggregates in Mn-doped ZnS nanobelts

Abstract: Tunable emission from the visible to infrared region in II–VI semiconductor nanostructures makes them ideal candidates for the development of optoelectronic devices.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

8
21
0

Year Published

2018
2018
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 37 publications
(29 citation statements)
references
References 53 publications
8
21
0
Order By: Relevance
“…Note that most reports in the literature refer to doped samples with the zinc blende structure. Papers related to the wurtzite structure are less frequent, and the stabilization of this high-temperature phase is mainly correlated with the formation of special elongated morphologies[8,15,16,[39][40][41]. However, in our case, the wurtzite phase was obtained due to the high temperatures reached during the MSR process.…”
mentioning
confidence: 58%
See 1 more Smart Citation
“…Note that most reports in the literature refer to doped samples with the zinc blende structure. Papers related to the wurtzite structure are less frequent, and the stabilization of this high-temperature phase is mainly correlated with the formation of special elongated morphologies[8,15,16,[39][40][41]. However, in our case, the wurtzite phase was obtained due to the high temperatures reached during the MSR process.…”
mentioning
confidence: 58%
“…Mn-doped ZnS is frequently synthesized by low temperature solution-based methods (precipitation, microemulsion, sol-gel, hydrothermal, reverse micelle…) [11][12][13][14] or evaporation processes (thermal evaporation, chemical vapor deposition…) [15,16]. These methods have some disadvantageous, such as high chemical complexity, the use of expensive chemical reagents, the need for prolonged reaction time and/or high pressure conditions.…”
Section: Introductionmentioning
confidence: 99%
“…6a for CdS Q-dots. The peak at 587nm corresponds to a characteristic emission of Mn 2+ ions (E Mn ~2.12 eV) between the 4 T 1 and 6 A 1 levels in the Mn 2+ doped CdS NPs [29,30]. Furthermore, it is evident that the emission peak in the glass samples heat treated at 575 o C and 600 o C are shifted to much longer wavelengths in Mn 2+ -doped CdS in Fig.…”
Section: Resultsmentioning
confidence: 99%
“…5 Many factors could affect their optical or magnetic properties, including the temperature, 4,6 dopant location 7,8 and composition/dopant concentration. 4,[9][10][11][12][13][14][15] As is well known, the composition is a key factor affecting the bandgaps of semiconductor nanomaterials, [16][17][18][19][20][21][22][23] e.g. the ternary Zn x Cd 1Àx S [16][17][18] , CdS x Se 1Àx 19 and ZnSe x Te 1Àx 20 nanowires, all showed the tunable bandgaps versus the composition.…”
Section: Introductionmentioning
confidence: 99%