2015
DOI: 10.1016/j.apsusc.2014.12.029
|View full text |Cite
|
Sign up to set email alerts
|

Interfacial interaction between the epoxidized natural rubber and silica in natural rubber/silica composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

4
122
0

Year Published

2015
2015
2023
2023

Publication Types

Select...
6
1

Relationship

3
4

Authors

Journals

citations
Cited by 154 publications
(126 citation statements)
references
References 30 publications
4
122
0
Order By: Relevance
“…Therefore, ENR is employed to improve the interaction between NR and silica and has been proved efficient. 10 As known, the chemical crosslink density represents the chemical molecular chain trapped in the matrix, while the physical crosslink density represents the entangled molecular chains of the rubber matrix. On the other hand, the chemical crosslink density can also reflect the interaction between rubber matrix and filler.…”
Section: Payne Effectmentioning
confidence: 99%
See 2 more Smart Citations
“…Therefore, ENR is employed to improve the interaction between NR and silica and has been proved efficient. 10 As known, the chemical crosslink density represents the chemical molecular chain trapped in the matrix, while the physical crosslink density represents the entangled molecular chains of the rubber matrix. On the other hand, the chemical crosslink density can also reflect the interaction between rubber matrix and filler.…”
Section: Payne Effectmentioning
confidence: 99%
“…Mechanism of interaction between ENR and silica. 10,12 ARTICLE WILEYONLINELIBRARY.COM/APP cavity temperature of 30 8C, and it was used to evaluate the anticompression properties of the composites.…”
Section: Characterizationmentioning
confidence: 99%
See 1 more Smart Citation
“…1 was the FTIR curves of ENR40/P-silica compounds that hadn't been cured. From the infrared spectrum of P-silica, 1108 cm -1 peak arises from Si-O-Si asymmetrical stretching vibration and the absorption peak at 804cm -1 is the symmetrical stretching vibration of Si-O [11] . In ENR40/P-silica compounds, 872 cm -1 and 832 cm -1 stand for the asymmetrical stretching vibration of epoxy ring.…”
Section: Advances In Intelligent Systems Research Volume 154mentioning
confidence: 99%
“…The epoxy group of ENR is unstable that could be utilized for the modification of ENR or being a compatilizer [3,4] in rubber composites. It is well known that SiO 2 is used widely in industry except for carbon black, usually as a reinforcement agent or a functionalized filler to impart specific properties for rubber compounds [5].…”