“…In the DTG curve, it is possible to see the degradation peak corresponding to this process, which can be assigned to some residual organic material from the synthesis. [175][176][177] The main weight loss occurs between 400 and 650°C due to the carbon decomposition. [177] For each material, the curves reach stability in The results shows that the more PtCl6 2 we added, more intense are the peaks corresponding to AgCl, Pt and PtO.…”