Influence of the solvent on the structure, morphology and performance for H2 evolution of CdS photocatalysts prepared by solvothermal method

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

3
47
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 162 publications
(54 citation statements)
references
References 95 publications
3
47
0
Order By: Relevance
“…As can be seen in Figure 4b,t he XPS peaks of the S2pl ocated at 161.37 and 162.47 eV are in accordance with the 2p 1/2 and2 p 3/2 of S 2À in CdS LDH .T hese results suggestt he successful formation of CdS. [37] Besides that, the element Al is also detected, with a binding energy of 74.95 eV (Figure 4c). This is consistent with our design that the amorphous aluminam atrix remains with the formation of CdS LDH during the sulfurationprocess.…”
Section: Xps Analysissupporting
confidence: 65%
See 1 more Smart Citation
“…As can be seen in Figure 4b,t he XPS peaks of the S2pl ocated at 161.37 and 162.47 eV are in accordance with the 2p 1/2 and2 p 3/2 of S 2À in CdS LDH .T hese results suggestt he successful formation of CdS. [37] Besides that, the element Al is also detected, with a binding energy of 74.95 eV (Figure 4c). This is consistent with our design that the amorphous aluminam atrix remains with the formation of CdS LDH during the sulfurationprocess.…”
Section: Xps Analysissupporting
confidence: 65%
“…As can be seen in Figure b, the XPS peaks of the S 2p located at 161.37 and 162.47 eV are in accordance with the 2p 1/2 and 2p 3/2 of S 2− in CdS LDH . These results suggest the successful formation of CdS . Besides that, the element Al is also detected, with a binding energy of 74.95 eV (Figure c).…”
Section: Resultsmentioning
confidence: 69%
“…Figure b contains the spectra of C1s; the peaks located at 284.1, 284.4, and 288.3 eV are attributed to contributions of sp 2 C=C bonds, sp 3 C–C bonds, and C=O bonds, respectively. As illustrated in Figure c, two peaks situated at 404.5 and 411.3 eV can be detected, which correspond to the Cd 3d 5/2 and Cd 3d 3/2 photoelectrons of the Cd 2+ species in CdS, respectively. The S 2p of this sample can be decomposed into two Gaussian peaks with binding energies at 161.3 and 162.1 eV (Figure [d]).…”
Section: Resultsmentioning
confidence: 93%
“…In this work, a facile solvothermal methodology was devised to prepare the HBSMs with a mixed solvent of GC and IP (1 : 1, v : v). As is well known, the solvents generally render certain effects on the crystal growth and even phase composition of a semiconductor over the solvothermal process [32][33][34]. To this end, the GC or IP was also adopted as a single solvent to synthesize BiOBr samples, as depicted in Table 1.…”
Section: Structural and Physicochemical Characterizationsmentioning
confidence: 99%