2008
DOI: 10.1016/j.dental.2007.10.001
|View full text |Cite
|
Sign up to set email alerts
|

Influence of pH on slow crack growth of dental porcelains

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2

Citation Types

0
43
0
3

Year Published

2010
2010
2022
2022

Publication Types

Select...
6
1
1

Relationship

0
8

Authors

Journals

citations
Cited by 50 publications
(46 citation statements)
references
References 27 publications
0
43
0
3
Order By: Relevance
“…In addition, previous studies have reported that the size of the leucite particles in feldspathic-based ceramics increased during heat treatment within the normal ceramic firing range 31,32) , thereby further increasing the probability of microcracking 33,34) . On the effect of pH of storage media on slow crack growth of dental porcelains, Pinto et al 35) concluded that leucite-based ceramic (as opposed to ceramic without leucite particles) was more susceptible to slow crack growth in acidic conditions compared to base and neutral conditions. This could thus explain why immersion in acidic agents had deleterious effects on IPS d.SIGN fluorapatite-leucite ceramic.…”
Section: Discussionmentioning
confidence: 99%
“…In addition, previous studies have reported that the size of the leucite particles in feldspathic-based ceramics increased during heat treatment within the normal ceramic firing range 31,32) , thereby further increasing the probability of microcracking 33,34) . On the effect of pH of storage media on slow crack growth of dental porcelains, Pinto et al 35) concluded that leucite-based ceramic (as opposed to ceramic without leucite particles) was more susceptible to slow crack growth in acidic conditions compared to base and neutral conditions. This could thus explain why immersion in acidic agents had deleterious effects on IPS d.SIGN fluorapatite-leucite ceramic.…”
Section: Discussionmentioning
confidence: 99%
“…Shorter storage in acid pH did not cause surface changes [4], but after 7 days of acid immersion, surface deterioration could be observed [1,2], with numerous porosities and small cracks covering the feldspathic ceramic surface [2]. This surface alteration could reduce the ceramic's flexural strength, although the crack growth rates of existing flaws were similar over time, regardless of the salivary pH [3]. Furthermore, the hardness of feldspathic ceramic could decrease with an increase in the pH [3], but this might not be responsible for the decrease in flexural strength, since storage in basic and neutral pH showed no influence on the present data.…”
Section: Discussionmentioning
confidence: 99%
“…Although ceramics are considered to be the most inert of all dental materials used for restorations [1], in reality, some ceramics are not chemically inert, even in a neutral aqueous environment [2], and storage in acid or basic pH can result in degradation of their flexural strength [1,3].…”
mentioning
confidence: 99%
“…Dez corpos-de-prova de cada grupo foram testados para cada taxa de tensão (Pinto et al, 2008;Rosa et al, 2009). Com exceção da taxa de 1 MPa/s, em que 30 barras foram ensaiadas para realizar a análise estatística de…”
Section: Análise De Weibull E Comportamento De Crescimento Subcríticounclassified
“…A literatura apresenta valores de n variando de 15 a 41 para porcelanas (Morena et al, 1986;Fairhurst et al, 1993;Pinto et al, 2008;Gonzaga et al, 2009;Rosa et al, 2009). Esses valores são semelhantes aos valores obtidos para vidros de silicato (15 a 19), que estão entre os materiais cerâmicos mais susceptíveis ao SCG (Ritter, 1978;Gupta;Jubb, 1981).…”
Section: Comportamento De Crescimento Subcrítico De Trincas -Scgunclassified