2014
DOI: 10.1016/j.solmat.2013.09.026
|View full text |Cite
|
Sign up to set email alerts
|

Influence of microstructure on temperature-induced ageing mechanisms of different solar absorber coatings

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
14
0
2

Year Published

2015
2015
2022
2022

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 37 publications
(17 citation statements)
references
References 54 publications
1
14
0
2
Order By: Relevance
“…Significant deviations in the absorption spectrum were observed after annealing nanocomposite absorber coating at 1273 K for 24 h. It has been shown that changes in the top surface morphology can be responsible for variation in the radiative properties at high temperatures. [ 41 ] In our case, the AFM surface profile image confirms the change in top surface morphology in terms of surface roughness and average particle size upon high‐temperature annealing (Figure S9, Supporting Information). The RMS values increased from 1–2 nm to 8–10 nm, and the average particle size increased from ≈5 nm to 35–40 nm.…”
Section: Resultssupporting
confidence: 71%
“…Significant deviations in the absorption spectrum were observed after annealing nanocomposite absorber coating at 1273 K for 24 h. It has been shown that changes in the top surface morphology can be responsible for variation in the radiative properties at high temperatures. [ 41 ] In our case, the AFM surface profile image confirms the change in top surface morphology in terms of surface roughness and average particle size upon high‐temperature annealing (Figure S9, Supporting Information). The RMS values increased from 1–2 nm to 8–10 nm, and the average particle size increased from ≈5 nm to 35–40 nm.…”
Section: Resultssupporting
confidence: 71%
“…In addition, the adhesion of solar absorbers is very important for flexible solar absorber applications. A solar absorber is usually used in complex and harsh environments, accompanied by delamination and stripping of coatings, and these problems are more severe for thick multilayered coatings . Therefore, overcoming the challenge of designing ultrathin SSACs by a simple method with excellent solar absorptivity and robust stability is of great importance for the practical application of flexible and wearable energy‐related devices.…”
Section: Introductionmentioning
confidence: 99%
“…Na amostra 3, não foi observado descolamento do filme, que apresentou-se também bastante homogêneo, entretanto foram observadas o surgimento de partículas esféricas depositadas sobre o filme. Kotilainen et al (2014) observaram o aparecimento de pequenas ilhas de óxido, em superfícies seletivas de cromo, depositadas sobre um substrato de cobre. Essas ilhas resultam da difusão de átomos do substrato para a superfície, devido ao processo de envelhecimento.…”
Section: Microscopia Eletrônica De Varreduraunclassified