Influence of annealing temperature on the spectroscopic properties of hydroxyapatite analogues doped with Eu3+

Abstract: Nanosized calcium and strontium hydroxyapatites doped with 2 mol% Eu3+ ions were obtained by using a microwave-assisted hydrothermal method.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

1
24
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 23 publications
(25 citation statements)
references
References 36 publications
1
24
0
Order By: Relevance
“…Two different types of crystallographic sites of Sr 2+ ions in hydroxyapatite lattice are current: four at the Sr(1) site with C 3 point symmetry situated on the ternary axes and six at the Sr(2) site with C S symmetry [ 30 , 31 ]. Moreover, in apatite structure, cis and trans symmetry of C S crystallographic site correlated with arrangements of Eu 3+ ions along the channel is well-known [ 8 ]. In the Sr 3 (PO 4 ) 2 matrix, there are two nonequivalent crystallographic sites of Sr 2+ ions: three at the Sr(1) site and six at the Sr(2) site.…”
Section: Resultsmentioning
confidence: 99%
See 4 more Smart Citations
“…Two different types of crystallographic sites of Sr 2+ ions in hydroxyapatite lattice are current: four at the Sr(1) site with C 3 point symmetry situated on the ternary axes and six at the Sr(2) site with C S symmetry [ 30 , 31 ]. Moreover, in apatite structure, cis and trans symmetry of C S crystallographic site correlated with arrangements of Eu 3+ ions along the channel is well-known [ 8 ]. In the Sr 3 (PO 4 ) 2 matrix, there are two nonequivalent crystallographic sites of Sr 2+ ions: three at the Sr(1) site and six at the Sr(2) site.…”
Section: Resultsmentioning
confidence: 99%
“…The decay profiles and the lifetime values are alike to each other and only minor differences were observed. The decay times of Eu 3+ ions in Sr 10 (PO 4 ) 6 (OH) 2 –Sr 3 (PO 4 ) 2 are typical for this kind of ion and are longer than for strontium apatite [ 7 , 8 ], which is caused by the presence of Sr 3 (PO 4 ) 2 phase.…”
Section: Resultsmentioning
confidence: 99%
See 3 more Smart Citations