In-situ X-ray diffraction study of stress-induced phase transition of (1 − x)BaZr0.2Ti0.8O3–xBa0.7Ca0.3TiO3 in polymer matrix composite

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3

Citation Types

0
6
0

Year Published

2015
2015
2023
2023

Publication Types

Select...
4

Relationship

2
2

Authors

Journals

citations
Cited by 4 publications
(6 citation statements)
references
References 26 publications
0
6
0
Order By: Relevance
“…32 The large d 33 value of BZT-0.5BZT/ZO 3step sample could also lead to the domain patterns remnant polarization. And in that case, we suggest the domain reorientation of T phase domain 5,28 is the main reason that the BZT-0.5BCT/ZO 3step sample has the largest d 33 value. In addition, from the normalized XRD in Fig.…”
Section: Resultsmentioning
confidence: 77%
See 2 more Smart Citations
“…32 The large d 33 value of BZT-0.5BZT/ZO 3step sample could also lead to the domain patterns remnant polarization. And in that case, we suggest the domain reorientation of T phase domain 5,28 is the main reason that the BZT-0.5BCT/ZO 3step sample has the largest d 33 value. In addition, from the normalized XRD in Fig.…”
Section: Resultsmentioning
confidence: 77%
“…5,31 And in that condition, the O-T phase transition and reorientation of T phase domain are becoming easier for BZT-0.5BCT, lead to a large d 33 value. 1,24,28,31 As shown in Fig. 5a, the d 33 value of BZT-0.5BCT/ZO 2step is the lowest among the three ceramics.…”
Section: Resultsmentioning
confidence: 78%
See 1 more Smart Citation
“…The CTE of SBT can reach as low as −150 × 10 −6  K −1 when the ferroelectric–paraelectric (tetragonal–cubic) phase transformation takes place222324. On the one hand, the Curie temperature ( T C ) of SBT is in the range of approximately 20 to 400 K, which can be precisely controlled by adjusting the Sr content22, suggesting that we can obtain large negative CTE in a temperature range near room temperature by using SBT powders with different Sr contents.…”
mentioning
confidence: 99%
“…Consequently, the dependence of the CTE of the SBT/Cu composite on the temperature can be designed by the Sr content. On the other hand, the Curie temperature of SBT is very sensitive to the stress23, and a thermal mismatch stress is an intrinsic feature of MMCs25. Therefore, a wide temperature range is expected for phase transformation owing to the non-uniform stress acting on the SBT particles with different sizes and shapes in the SBT/Cu composite.…”
mentioning