Improvement in strength of the aluminium/epoxy bonding joint by modification of the interphase

Abstract: This contribution describes the influence of different surface pre-treatments in cluding self-assembly of phosphoric acid mono alkyl ester as adhesion promoter (AP) for adhesive bonding of aluminium alloy AlMg3. The investigations were performed using a cold hardening two components epoxy-adhesive. The pre-treated surfaces, the interphase structures and the joints were characterized by: SEM/EDX, surface tension, XPS, DMA and the determination of mechanical parameters. The results interestingly show that the te… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
5
0

Year Published

2005
2005
2017
2017

Publication Types

Select...
7

Relationship

2
5

Authors

Journals

citations
Cited by 11 publications
(5 citation statements)
references
References 0 publications
0
5
0
Order By: Relevance
“…With AAO coated titanium, the composition of the interface shows mixing between the two components,42 which might suggest a bond between AAO and titanium substrate which is less reliant on keying between the coating and the substrate roughness/porosity. It is worth noting that under certain conditions AAO coatings can be produced on aluminum substrates with shear strength of the interface in excess of 40 MPa 43…”
Section: Discussionmentioning
confidence: 99%
“…With AAO coated titanium, the composition of the interface shows mixing between the two components,42 which might suggest a bond between AAO and titanium substrate which is less reliant on keying between the coating and the substrate roughness/porosity. It is worth noting that under certain conditions AAO coatings can be produced on aluminum substrates with shear strength of the interface in excess of 40 MPa 43…”
Section: Discussionmentioning
confidence: 99%
“…Most of them use this technique for evaluating the curing of thermosets [8][9][10] as an alternative to differential scanning calorimetry. Influence of environmentally induced ageing [11,12] or specific parameters to bonding process, like surface pretreatment of substrates [13,14], is also investigated.…”
Section: Introductionmentioning
confidence: 99%
“…1 The latter is the preferred oxide structure for adhesive bonding because of its mechanical stability and the highly porous layer structure. 7,8 Cleaning not only improves wetting but can also enhance the adhesive properties of the oxide layer. 6 Therefore, mostly wet (electro)chemical processes (etching, anodizing) are used.…”
Section: Introductionmentioning
confidence: 99%