Hydration and glass transition of hybrid non-isocyanate polyurethanes with POSS inclusions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
4
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 15 publications
(12 citation statements)
references
References 79 publications
1
4
0
Order By: Relevance
“…The loss of mechanical performance of our NIPUs in the hydrated state may be related to moisture-induced plasticization primarily caused by the presence of those –OH groups, as described for NIPU-based materials. 44–46 A drop in Young's modulus is usually accompanied by a decrease in σ r , which was observed in our NIPU samples. However, in contrast to Pronoitis et al , 45 an increase in ε r was not observed neither for PPG-NIPU nor for PTHF-NIPU.…”
Section: Discussionsupporting
confidence: 75%
“…The loss of mechanical performance of our NIPUs in the hydrated state may be related to moisture-induced plasticization primarily caused by the presence of those –OH groups, as described for NIPU-based materials. 44–46 A drop in Young's modulus is usually accompanied by a decrease in σ r , which was observed in our NIPU samples. However, in contrast to Pronoitis et al , 45 an increase in ε r was not observed neither for PPG-NIPU nor for PTHF-NIPU.…”
Section: Discussionsupporting
confidence: 75%
“…The resulting values for and were 0.63 ± 0.071 and 0.918 ± 0.004, respectively. The parameter exhibits a rather low value compared to the values reported in the literature for similar systems [ 67 , 68 ]; however, it remains in the range characteristic for Brunauer type III isotherms [ 70 ]. The parameter is close to 1.0 and of the value is usually reported for the materials exhibiting Brunauer type III behavior [ 67 , 68 ].…”
Section: Resultsmentioning
confidence: 82%
“…The parameter exhibits a rather low value compared to the values reported in the literature for similar systems [ 67 , 68 ]; however, it remains in the range characteristic for Brunauer type III isotherms [ 70 ]. The parameter is close to 1.0 and of the value is usually reported for the materials exhibiting Brunauer type III behavior [ 67 , 68 ]. The closer the parameter is to unity, the more similar the behavior of the formed multilayers is to the behavior of liquid water [ 71 ].…”
Section: Resultsmentioning
confidence: 82%
See 1 more Smart Citation
“…[55,71,72,[93][94][95] Thus, syntheses of thermosetting PHUs are generally carried out at high temperatures, that is, T ≥ 70 °C, in order to promote the homogenization of the monomers and the carbonate-amine reaction. [9][10][11][12][13][14][15][16][17]20,23,[25][26][27][28][29]31,32,36,38,39,45,68,[96][97][98][99][100][101][102][103] However, the following part of this literature review shows that an increasing number of references are reporting the synthesis of PHU networks at low temperatures, using several of the levers previously mentioned. Arbitrarily, the limit to discriminate the high-from the low-temperature curable systems was set at 70 °C.…”
Section: Preamblementioning
confidence: 99%