Hot deformation behavior and microstructure evolution of Mg-Gd-Y(-Sm)-Zr alloys

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
7
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 29 publications
(7 citation statements)
references
References 55 publications
0
7
0
Order By: Relevance
“…As the strain increases, the DRXed grains grow, and its average grain size gradually increases from ~10.6 to 13.9 µm, as seen in Figure 11e,f. Generally, the DRX process plays a key role in refining the grains and weakening the basal texture [43,45]. The DRX area shows a lower basal pole intensity than the whole one in the (0001) pole figures for the 0.3 and 0.5 strains (see Figure 11g,h).…”
Section: Hot Processing Map During Hot Compressionmentioning
confidence: 95%
See 1 more Smart Citation
“…As the strain increases, the DRXed grains grow, and its average grain size gradually increases from ~10.6 to 13.9 µm, as seen in Figure 11e,f. Generally, the DRX process plays a key role in refining the grains and weakening the basal texture [43,45]. The DRX area shows a lower basal pole intensity than the whole one in the (0001) pole figures for the 0.3 and 0.5 strains (see Figure 11g,h).…”
Section: Hot Processing Map During Hot Compressionmentioning
confidence: 95%
“…In order to describe the DRX kinetics model, in general, the following equation can be used and expressed [43,44]:…”
Section: Drx Kinetics During Hot Compressionmentioning
confidence: 99%
“…Different twinning systems have been observed in deformed Mg and Mg alloys, and the most common one is the {1012} twinning system [18][19][20]. Theoretically, {1012} deformation twin has six equivalent variants denoted as Ti (i = 1 .…”
Section: Introductionmentioning
confidence: 99%
“…Different twinning systems have been observed in deformed Mg and Mg alloys, and the most common one is the twinning system [18-20]. Theoretically, deformation twin has six equivalent variants denoted as Ti (i = 1 … 6) and these multiple twin variants can be initiated simultaneously and interact with each other [21-24].…”
Section: Introductionmentioning
confidence: 99%
“…The effect of samarium on magnesium alloys with yttrium and gadolinium was investigated in [35][36][37][38][39]. In works [35,36], alloys with a high content of gadolinium were considered.…”
Section: Introductionmentioning
confidence: 99%