High Throughput Wet Etch Solution for BEOL TiN Removal

Abstract: Sub-10 nm technology node manufacturing processes may require the use of thicker and denser TiN hard mask for patterning at the BEOL. The modified TiN, which tends to be more chemically robust, must be removed using a wet etch process, while maintaining typical throughput - no extension of typical wet etch process times. To satisfy these needs, a new TiN etching accelerator was found that enhanced the activity of peroxide-related species in a wet etch chemical formulation that achieved increased TiN etch rate … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Publication Types

Select...

Relationship

0
0

Authors

Journals

citations
Cited by 0 publications
references
References 4 publications
0
0
0
Order By: Relevance

No citations

Set email alert for when this publication receives citations?