High strain rate superplasticity of a Zn–22wt.%Al–xwt.%Ag alloys

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
6
0
3

Year Published

2008
2008
2021
2021

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 13 publications
(9 citation statements)
references
References 20 publications
(23 reference statements)
0
6
0
3
Order By: Relevance
“…This phase corresponds to a stable Agcontaining (AgCu)Zn 4 ¾ Ag phase which inhibits the four-phase reaction and it was reported as the º phase. 16) Thus, the aged ZACA2 alloy has a mixture of both the ¾ and Agcontaining ¾ Ag phases. That is, the ¾ phase reacts with the © phase to form the¸A phase and the Ag-containing ¾ Ag phase remains unchanged which is detected by the presence of XRD peaks corresponding to a cph phase.…”
Section: Xrd Characterization Of Alloysmentioning
confidence: 99%
See 1 more Smart Citation
“…This phase corresponds to a stable Agcontaining (AgCu)Zn 4 ¾ Ag phase which inhibits the four-phase reaction and it was reported as the º phase. 16) Thus, the aged ZACA2 alloy has a mixture of both the ¾ and Agcontaining ¾ Ag phases. That is, the ¾ phase reacts with the © phase to form the¸A phase and the Ag-containing ¾ Ag phase remains unchanged which is detected by the presence of XRD peaks corresponding to a cph phase.…”
Section: Xrd Characterization Of Alloysmentioning
confidence: 99%
“…There are several works which have analyzed the effect of addition of silver to the ZnAl and ZnAlCu alloys. 1416) For instance, Casolco et al 15,16) reported that the Ag addition between 4 and 6.15 mass% to the Zn22 mass%Al alloy caused the formation of an intermetallic compound AgZn 3 with a hcp crystalline structure. Additionally, the addition of about 1 Ag mass% to the Zn22 mass%Al alloy has been observed 14) to produce a strong grain refinement of the ¡ and © phases.…”
Section: Introductionmentioning
confidence: 99%
“…En el envejecimiento, los picos característicos de la fase ε desaparecen después de 5 horas y aparecen los picos de difracción de la fase τ'. La descomposición de la fase ε y la aparición de la fase τ', ha sido asociado con la reacción de cuatro fases α + ε→η + τ' (Hillert, 1998) y es la responsable de la inestabilidad dimensional de la aleación (Murphy, 1975;Mykura et al, 1986;Zhu, 1999;Casolco et al, 2006). Después de 10 horas a 200 °C se obtienen las fases de equilibrio η, α y τ' (Baker, 1992;Zhu, 2004).…”
Section: Caracterización Mediante Difracción De Rayos Xunclassified
“…Los picos de difracción de rayos X correspondientes a la fase Φ fueron identificados mediante la ficha PDF 51-0642 con una composición (Cu,Ag)Zn 4 . Es decir, la adición de Ag promueve la formación de la fase Φ con una estructura hcp (Casolco et al, 2003;Casolco et al, 2006). La Figura 1b muestra la evolución de los diagramas de difracción de rayos X de la aleación Zn-22%Al-2%Cu-1%Ag.…”
Section: Caracterización Mediante Difracción De Rayos Xunclassified
See 1 more Smart Citation