High Reactive MgO‐Y2O3 Nanopowders via Microwave Combustion Method and Sintering Behavior

Abstract: To decrease the sintering temperature of MgO-Y 2 O 3 composites to avoid undesired grain coarsening, high reactive MgO-Y 2 O 3 nanopowders were synthesized via microwave combustion method. The degree of combustion was enhanced effectively by adding an extra oxidant ammonium nitrate. The as-synthesized MgO-Y 2 O 3 nanopowders,~18 nm in size, showed high specific surface area of 64.55 m 2 /g and low agglomeration. Relative density of 98% was obtained when sintered at a low sintering temperature of 1350°C. The hi… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2017
2017
2023
2023

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 11 publications
(3 citation statements)
references
References 24 publications
(22 reference statements)
0
3
0
Order By: Relevance
“…The transformation of nano-Fe 2 O 3 to a-Fe could be attributed to the formation of inner reductive atmosphere of hydrocarbons and hydrogen (C x H y , H 2 ) during the pyrolysis process. [14][15][16] According to the Scherrer equation, 17 the size of a-Fe crystallites and graphite could be calculated to be about 35 nm and 20 nm, indicating the simultaneous formation of a-Fe and graphite crystallite in the Fe-doped SiCN ceramics. Fig.…”
Section: Methodsmentioning
confidence: 99%
“…The transformation of nano-Fe 2 O 3 to a-Fe could be attributed to the formation of inner reductive atmosphere of hydrocarbons and hydrogen (C x H y , H 2 ) during the pyrolysis process. [14][15][16] According to the Scherrer equation, 17 the size of a-Fe crystallites and graphite could be calculated to be about 35 nm and 20 nm, indicating the simultaneous formation of a-Fe and graphite crystallite in the Fe-doped SiCN ceramics. Fig.…”
Section: Methodsmentioning
confidence: 99%
“…For the preparation of YM composite, ball milling has been used as a combination with other routes (above‐mentioned methods) but not as a single primary method 28–31 . Fabrication of YM composite using commercial powders by using only ball‐milling method eliminates an extra step in the synthesis process, saving time and reducing costs.…”
Section: Introductionmentioning
confidence: 99%
“…For the preparation of YM composite, ball milling has been used as a combination with other routes (above-mentioned methods) but not as a single primary method. [28][29][30][31] Fabrication of YM composite using commercial powders by using only ball-milling method eliminates an extra step in the synthesis process, saving time and reducing costs. The variations in ball milling parameters are mostly constrained to the milling speed and time, ballto-powder weight ratio, milling atmosphere, and temperature.…”
Section: Introductionmentioning
confidence: 99%