High-quality boron carbide nanowires prepared by catalyst-free template growth method

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
3
1

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(2 citation statements)
references
References 38 publications
0
2
0
Order By: Relevance
“…The intensity of the Si–O bond peak at 1000–1200 cm –1 increases with longer oxidation times of the Si, indicating an elevated in the SiO 2 content . The mass contents of SiO 2 and SiC are evaluated using the reference intensity (RIR) method, as shown in Figure e . The mass content of SiC is 88.88% in SiC@SiO 2 NWs-0, which decreases to 88.04, 76.16, and 74.47% in SiC@SiO 2 -5, SiC@SiO 2 -15, and SiC@SiO 2 -30, respectively.…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…The intensity of the Si–O bond peak at 1000–1200 cm –1 increases with longer oxidation times of the Si, indicating an elevated in the SiO 2 content . The mass contents of SiO 2 and SiC are evaluated using the reference intensity (RIR) method, as shown in Figure e . The mass content of SiC is 88.88% in SiC@SiO 2 NWs-0, which decreases to 88.04, 76.16, and 74.47% in SiC@SiO 2 -5, SiC@SiO 2 -15, and SiC@SiO 2 -30, respectively.…”
Section: Resultsmentioning
confidence: 99%
“…48 The mass contents of SiO 2 and SiC are evaluated using the reference intensity (RIR) method, as shown in Figure 4e. 49 The mass content of SiC is 88.88% in SiC@SiO 2 NWs-0, which decreases to 88.04, 76.16, and 74.47% in SiC@SiO 2 -5, SiC@SiO 2 -15, and SiC@SiO 2 -30, respectively. This finding aligns with the FTIR results.…”
Section: Acs Sustainable Chemistry and Engineeringmentioning