2009
DOI: 10.1134/s1995421209030101
|View full text |Cite
|
Sign up to set email alerts
|

Fractography of degradation surfaces of adhesive joints after high-temperature thermal aging

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
1
0

Year Published

2019
2019
2021
2021

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(1 citation statement)
references
References 0 publications
0
1
0
Order By: Relevance
“…[8,9] The design service life of automobiles often exceeds several decades, which puts forward higher requirements for the reliability and durability of adhesive structure. [10][11][12] Currently, the interfacial bonding strength has been widely studied as a criterion to evaluate the bonding properties of heterogeneous materials. For the cemented structure, there are relatively many factors that affect its strength.…”
mentioning
confidence: 99%
“…[8,9] The design service life of automobiles often exceeds several decades, which puts forward higher requirements for the reliability and durability of adhesive structure. [10][11][12] Currently, the interfacial bonding strength has been widely studied as a criterion to evaluate the bonding properties of heterogeneous materials. For the cemented structure, there are relatively many factors that affect its strength.…”
mentioning
confidence: 99%