2014
DOI: 10.1016/j.physb.2014.05.012
|View full text |Cite
|
Sign up to set email alerts
|

Formation of MgZnO alloy under thermodynamic conditions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
8
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 7 publications
(9 citation statements)
references
References 25 publications
1
8
0
Order By: Relevance
“…The revealed peak shifts indicate formation of ZnMgO solid solutions of hexagonal and cubic crystalline structures. In fact, we have shown earlier that formation of cubic and hexagonal ZnMgO phases occurs side by side during sintering of ZnMgO ceramics. The concentrations of the hexagonal ZnO‐like and cubic MgO‐like crystal phases evaluated by Reference Intensity Ratio method were found to be, respectively, 94 and 6% in the films annealed at temperatures in the range of 800–1000 °C and 96 and 4% in the films annealed at lower temperatures.…”
Section: Resultsmentioning
confidence: 80%
See 1 more Smart Citation
“…The revealed peak shifts indicate formation of ZnMgO solid solutions of hexagonal and cubic crystalline structures. In fact, we have shown earlier that formation of cubic and hexagonal ZnMgO phases occurs side by side during sintering of ZnMgO ceramics. The concentrations of the hexagonal ZnO‐like and cubic MgO‐like crystal phases evaluated by Reference Intensity Ratio method were found to be, respectively, 94 and 6% in the films annealed at temperatures in the range of 800–1000 °C and 96 and 4% in the films annealed at lower temperatures.…”
Section: Resultsmentioning
confidence: 80%
“…The phase diagram of ZnO‐MgO binary system predicted a pure wurtzite Zn 1‐x Mg x O alloy with Mg content up to about 4% . The solubility limit of Mg in hexagonal Zn 1‐x Mg x O alloy produced under thermodynamic conditions has been shown to be about 20%, although formation of the hexagonal and cubic ZnMgO phases occurs simultaneously . In the films grown under metastable conditions, pure wurtzite Zn 0.6 Mg 0.4 O phase has been reported .…”
Section: Introductionmentioning
confidence: 99%
“…In this case, the samples were located in a closed crucible with metallic zinc scraps and annealed in N 2 flow. In all cases, firm and dense hexagonal phase ceramics were obtained (X-ray diffraction patterns were shown in [13]). Prepared samples were cut transversally and defect-related PL spectra in 400-800 nm range as well as PL excitation (PLE) spectra in 250-400 nm range were measured from cleft surface at room temperature.…”
Section: Methodsmentioning
confidence: 96%
“…The Mg content x was changed from 0 up to 0.20, which was found to be the solubility limit of Mg in hexagonal-structure Mg x Zn 1-x O ceramics [13]. After drying at room temperature, the samples were sintered in air at 1050 °C for 3 hours and cooled with the furnace.…”