Formability, mechanical and corrosive properties of Mg–Nd–Zn–Zr magnesium alloy seamless tubes

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
11
0

Year Published

2012
2012
2017
2017

Publication Types

Select...
4
3
2

Relationship

0
9

Authors

Journals

citations
Cited by 46 publications
(11 citation statements)
references
References 15 publications
0
11
0
Order By: Relevance
“…In addition, the precipitates in the DEAP alloy are smaller and distribute more uniformly than that in the OEAP alloy, which can effectively restrain the gliding of dislocation during tensile deformation. 26 Consequently, the improved yield strength of the EDAP can be ascribed to the grain refinement of both matrix and precipitated phase, and homogeneous microstructure. The yield strength of the OEAP and DEAP are improved by ∼18 and ∼10% respectively compared to those of the once and double extrusions without aging treatment according to our previous work, 24 and the elongation of the age treated alloys declines slightly.…”
Section: Mechanical Propertiesmentioning
confidence: 99%
“…In addition, the precipitates in the DEAP alloy are smaller and distribute more uniformly than that in the OEAP alloy, which can effectively restrain the gliding of dislocation during tensile deformation. 26 Consequently, the improved yield strength of the EDAP can be ascribed to the grain refinement of both matrix and precipitated phase, and homogeneous microstructure. The yield strength of the OEAP and DEAP are improved by ∼18 and ∼10% respectively compared to those of the once and double extrusions without aging treatment according to our previous work, 24 and the elongation of the age treated alloys declines slightly.…”
Section: Mechanical Propertiesmentioning
confidence: 99%
“…Moreover, the market price of Sm is much cheaper than that of Nd and Y [15]. It is, therefore, meaningful to produce low-price, heat-resistant Mg-Sm alloys with proper mechanical properties to compete with traditional Mg-RE alloys [16][17][18].…”
Section: Introductionmentioning
confidence: 99%
“…%) and low solubility at room temperature (~ 100 ppm), which make it suitable for potential age hardening [8]. The strength of age-hardened Mg-Nd alloys can be further enhanced through solid solution strengthening by controlled addition of third element such as zinc (Zn) [9,[10][11][12][13][14]. Researches have shown that addition of 0.2 wt.…”
Section: Introductionmentioning
confidence: 99%
“…% Zn to Mg-3 Nd wt. % alloy improves the mechanical properties through mainly solid solution strengthening mechanism [8,[12][13][14][15][16][17][18][19].…”
Section: Introductionmentioning
confidence: 99%