2020
DOI: 10.1016/j.jallcom.2020.153695
|View full text |Cite
|
Sign up to set email alerts
|

Fe-based metallic glass reinforced FeCoCrNiMn high entropy alloy through selective laser melting

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
19
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 45 publications
(19 citation statements)
references
References 28 publications
0
19
0
Order By: Relevance
“…Spontaneous crystallization is normally inevitable. It is believed that die casting (10 1 -10 3 K s −1 ), [38] melt spinning (10 5 -10 6 K s −1 ), liquid splat-quenching (10 9 -10 10 K s −1 ), and pulse laser quenching (10 12 -10 13 K s −1 ) [71] cannot satisfy the supercooling requirements for the formation of single element MGs. Zhong et al reported a rapid quenching route with unprecedented high liquid quenching rate (10 14 K s −1 ) to obtain vitrified metallic element.…”
Section: Top-down Approachmentioning
confidence: 99%
“…Spontaneous crystallization is normally inevitable. It is believed that die casting (10 1 -10 3 K s −1 ), [38] melt spinning (10 5 -10 6 K s −1 ), liquid splat-quenching (10 9 -10 10 K s −1 ), and pulse laser quenching (10 12 -10 13 K s −1 ) [71] cannot satisfy the supercooling requirements for the formation of single element MGs. Zhong et al reported a rapid quenching route with unprecedented high liquid quenching rate (10 14 K s −1 ) to obtain vitrified metallic element.…”
Section: Top-down Approachmentioning
confidence: 99%
“…The parameters are different according to the powder composition, particle size, sphericity, and even the difference of equipment. According to most studies, the reasonable energy density is in the range of 30-100 J/mm 3 [50,79,80,[83][84][85][86]. Hofmann studied the effect of processing on the microstructure and properties of an FeCrMoBC glass-forming alloy through a variety of manufacturing parameters by SLM [74].…”
Section: Parameters Of Slmmentioning
confidence: 99%
“…In particular, the maximum fracture toughness of BMGCs after mixing with Cu particles reached 47 MPa m 1/2 , which is about 20 times higher than that of Fe-based BMG (2.2 MPa m 1/2 ). Interestingly, Li also used SLM technology to combine an iron-based highentropy alloy with an iron-based glass to produce a composite with both high strength and high toughness [79]. The strength and toughness of the composite can be effectively adjusted with the difference of metal glass content.…”
Section: Mechanical Properties Of Bmgsmentioning
confidence: 99%
“…Apart from SPS, SLM is the most widely studied AM technique for HEAs . HEAs that were successfully fabricated by SLM include CoCrFeNiMn [153,154,169,[176][177][178][179][180][181][182][183][184][185]188,[202][203][204][205][206]209,212,214,215,217,220,221], AlCrFeNiV [193], AlCoCrFeNi [170,190], Al-CoCrCuFeNi [194], CoCrFeNi [98,155,186,187,189,208,213,222], CoCr 2.5 FeNi 2 TiW 0.5 [223],…”
Section: Additive Manufacturing Of Heasmentioning
confidence: 99%
“…They have also shown that the properties of HEAs could be altered by changing the input parameters for AM process. For example, CoCrFeNiMn was manufactured with SLM by multiple researchers [153,154,169,[176][177][178][179][180][181][182][183][184][185]188,[202][203][204][205][206]209,212,214,215,217,220,221] and many of them acquired different mechanical properties for CoCrFeNiMn by changing input parameters in AM processes (refer Tables 1-3).…”
Section: Additive Manufacturing Of Heasmentioning
confidence: 99%