Fabrication of Al–20wt%Si powder using scrap Si by ultra high-energy milling process

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
8
0

Year Published

2014
2014
2024
2024

Publication Types

Select...
9
1

Relationship

0
10

Authors

Journals

citations
Cited by 27 publications
(12 citation statements)
references
References 12 publications
2
8
0
Order By: Relevance
“…4f and in accordance with the SEM results. Similar results are reported for Al-Si [44] and Cu-Al-Mn powder [45].…”
Section: Resultssupporting
confidence: 89%
“…4f and in accordance with the SEM results. Similar results are reported for Al-Si [44] and Cu-Al-Mn powder [45].…”
Section: Resultssupporting
confidence: 89%
“…3b). It has been reported that similar observations are obtained using EDX in previous paper by Won-Kyung Kang et al, for Al-20 wt%Si powder [18]. As it seen Fig.…”
Section: Microstructural Evaluationsupporting
confidence: 89%
“…[9] and the other is inability of milling time to form any intermetallic phases. [10]. Very long counting rates can be necessary to detect the presence any sizeable intermetallic signals but also the additional phases can be engaged in the any α-phases.…”
Section: Resultsmentioning