Experimental Evaluation of the Performance of Crystalline Si PV Module Degradation After 15-Years of Field Exposure

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
0
0
1

Year Published

2022
2022
2022
2022

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
(1 citation statement)
references
References 23 publications
0
0
0
1
Order By: Relevance
“…As plantas fotovoltaicas apresentam perdas esperadas durante o período de operação que afetam o seu desempenho. Sendo as mais comuns, as perdas ôhmicas nos cabeamentos (Nascimento e Ferreira, 2018), a sujeira, a degradação induzida pela luz (LID -Ligth Induced Degradation), Silva et al (2018), a degradação ao longo da vida útil dos módulos esperada de menos de 1% por ano Cassini et al (2018) e aquelas resultantes da temperatura de operação dos módulos. No inversor, as perdas ocorrem durante a conversão de energia de Corrente Contínua (CC) para Corrente Alternada (AC) (Nascimento e Ferreira, 2018).…”
Section: Introductionunclassified
“…As plantas fotovoltaicas apresentam perdas esperadas durante o período de operação que afetam o seu desempenho. Sendo as mais comuns, as perdas ôhmicas nos cabeamentos (Nascimento e Ferreira, 2018), a sujeira, a degradação induzida pela luz (LID -Ligth Induced Degradation), Silva et al (2018), a degradação ao longo da vida útil dos módulos esperada de menos de 1% por ano Cassini et al (2018) e aquelas resultantes da temperatura de operação dos módulos. No inversor, as perdas ocorrem durante a conversão de energia de Corrente Contínua (CC) para Corrente Alternada (AC) (Nascimento e Ferreira, 2018).…”
Section: Introductionunclassified