Evaluation of nickel-containing zeolites in the catalytic transformation of glucose in an aqueous medium

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
0
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 9 publications
(2 citation statements)
references
References 56 publications
0
0
0
Order By: Relevance
“…In the last case, glucose is spent almost entirely on the formation of humins. Their structure appears to be comparable to that proposed in the paper 26 on Nicontaining synthetic zeolites, but in the experiments without the catalyst glucose-ring fragments are predominant in the humin structures with lower content of furan rings (Fig. 3).…”
Section: Glucose Transformationsupporting
confidence: 82%
See 1 more Smart Citation
“…In the last case, glucose is spent almost entirely on the formation of humins. Their structure appears to be comparable to that proposed in the paper 26 on Nicontaining synthetic zeolites, but in the experiments without the catalyst glucose-ring fragments are predominant in the humin structures with lower content of furan rings (Fig. 3).…”
Section: Glucose Transformationsupporting
confidence: 82%
“…The reaction temperature was 433 K and was chosen based on the results of previous studies. 26 Samples of liquid products for analysis were taken every hour. In the case of experiments without a catalyst, 23 g of 20 % glucose solution in DMSO was used.…”
Section: Catalytic Testingmentioning
confidence: 99%