Enhancement of the crystalline perfection of <0 0 1> directed KDP single crystal

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

2
9
0

Year Published

2014
2014
2023
2023

Publication Types

Select...
9

Relationship

2
7

Authors

Journals

citations
Cited by 28 publications
(11 citation statements)
references
References 30 publications
2
9
0
Order By: Relevance
“…So, it is important to know the threshold intensities of the crystal can withstand without getting damaged [27]. High laser damage threshold is a significant parameter for NLO crystal.…”
Section: Laser Damage Threshold (Ldt)mentioning
confidence: 99%
See 1 more Smart Citation
“…So, it is important to know the threshold intensities of the crystal can withstand without getting damaged [27]. High laser damage threshold is a significant parameter for NLO crystal.…”
Section: Laser Damage Threshold (Ldt)mentioning
confidence: 99%
“…The hardness of the material depends on several parameters such as Debye temperature, lattice energy, heat of formation and inter-atomic spacing [26][27][28]. For load dependence of Vickers microhardness measurement, the indentation time was constant at 5 s. The diagonal lengths of the indented impression were measured for different loads varying from 5 to 200 g. The consecutive indentations were made at various sites of the sample surface.…”
Section: Vickers Microhardness Measurementmentioning
confidence: 99%
“…Therefore amino acids are found to be more efficient candidates as dopants in growing inorganic crystals. In our earlier papers more results have been found on h0 0 1i directed KDP [20] and glycine added KDP [21].…”
Section: Introductionmentioning
confidence: 86%
“…9 The laser damage threshold (LDT) of nonlinear optical components depends on physical and chemical factors, particularly imperfections, defects and the concentration and type of the impurities, etc. 10 The LDT of the grown pure and 2M%-K 2 CO 3 -doped KDP single crystals was carried out using a Nd:YAG laser with the wavelength 1064 nm and shot-to-shot mode, with an energy per pulse of 50 mJ, a repetition rate of 10 Hz, a pulse duration of 7 ns, a beam waist of 0.0841 mm and a spot diameter of 2.3 mm.…”
Section: Laser Damage Threshold (Ldt)mentioning
confidence: 99%