Enhanced toughness of hydroxyapatite–poly(ethylene terephthalate) composites by immersion in water

Abstract: Water-soluble poly(ethylene terephthalate) bearing carboxylate groups on 14-22% of the phenylene moieties was coprecipitated with calcium ion and phosphate ion in water at room temperature, 70 oC, and 90 oC...

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
6
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
5

Relationship

2
3

Authors

Journals

citations
Cited by 6 publications
(6 citation statements)
references
References 67 publications
(101 reference statements)
0
6
0
Order By: Relevance
“…Coprecipitation can be accomplished in one pot and in a large scale. Both water-soluble polymers , and amphiphilic polymers can be used for hybridization with coprecipitation. For instance, collagen, , chitosan, starch, , cellulose derivatives, , poly­(vinyl alcohol), , and polyacrylic acid , have been employed to hybridize with HAP.…”
Section: Introductionmentioning
confidence: 99%
“…Coprecipitation can be accomplished in one pot and in a large scale. Both water-soluble polymers , and amphiphilic polymers can be used for hybridization with coprecipitation. For instance, collagen, , chitosan, starch, , cellulose derivatives, , poly­(vinyl alcohol), , and polyacrylic acid , have been employed to hybridize with HAP.…”
Section: Introductionmentioning
confidence: 99%
“…Bending vibrations for PO 4 −3 groups appeared near 560 cm −1 and 602 cm −1 and similar spectra were noticed for all the gamma-irradiated HAp samples. 31 For the normal mode of ν 1 and ν 3 vibrations of the phosphate group, the most intense peak was visualized at the fingerprint region which is at the 1026 cm −1 wavenumber along with two accompanying peaks at 962 and 1095 cm −1 . The triple degenerate of ν 3 asymmetric stretching due to the phosphate group was noticed at the wavenumbers of 1026 and 1085 cm −1 .…”
Section: Resultsmentioning
confidence: 96%
“…Larger water absorption of Composite 2 carboxylates than that of Composite 1 carboxylates can be attributed to a larger pore volume of the composites having a larger inorganic volume fraction. 26 On the other hand, Composite 2 laurates showed similar water absorption to that of Composite 1 laurates when acylation temperature was higher than 100 °C (Figure S3). Flexible alkyl chains of laurate can fill the pore in the composite to prevent water penetration.…”
Section: ■ Results and Discussionmentioning
confidence: 99%
“…The values of water absorption Δ w / w (%) of Composite 2 acetate and Composite 2 benzoate were larger than those of the corresponding Composite 1. Larger water absorption of Composite 2 carboxylates than that of Composite 1 carboxylates can be attributed to a larger pore volume of the composites having a larger inorganic volume fraction . On the other hand, Composite 2 laurates showed similar water absorption to that of Composite 1 laurates when acylation temperature was higher than 100 °C (Figure S3).…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation