Energy-effective AlMgB14 production by self-propagating high-temperature synthesis (SHS) using the chemical furnace as a source of heat energy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
14
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
9

Relationship

3
6

Authors

Journals

citations
Cited by 17 publications
(14 citation statements)
references
References 14 publications
0
14
0
Order By: Relevance
“…It is also important to note that in addition to the AlB 12 phase, the Al 0.5 Mg 0.5 B 2 phase is formed in the obtained specimens. In [ 11 , 17 , 23 ], it was found that the Al 0.5 Mg 0.5 B 2 diboride phase is an intermediate phase in the formation of aluminum magnesium boride AlMgB 14 . However, the presence of an inert diluent (silicon) absorbs part of the heat energy and prevents the formation of the AlMgB 14 phase under the selected sintering mode, despite the completion of the specimen consolidation process.…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…It is also important to note that in addition to the AlB 12 phase, the Al 0.5 Mg 0.5 B 2 phase is formed in the obtained specimens. In [ 11 , 17 , 23 ], it was found that the Al 0.5 Mg 0.5 B 2 diboride phase is an intermediate phase in the formation of aluminum magnesium boride AlMgB 14 . However, the presence of an inert diluent (silicon) absorbs part of the heat energy and prevents the formation of the AlMgB 14 phase under the selected sintering mode, despite the completion of the specimen consolidation process.…”
Section: Resultsmentioning
confidence: 99%
“…The samples were found to have a friction coefficient below 0.2 when sliding against Si 3 N 4 , Al 2 O 3 , and SiC. In the last two decades, polycrystalline materials based on AlMgB 14 have been actively studied [ 9 , 10 , 11 ]. AlMgB 14 is also based on B 12 icosahedrons forming an orthorhombic structure, has high hardness (up to 32 GPa), and a low friction coefficient (COF, 0.08–0.02).…”
Section: Introductionmentioning
confidence: 99%
“…This leads to an increase in the combustion temperature of SHS powders. As the literature analysis shows, the optimum sintering temperature for AlMgB 14 is 1400 • C [1, 4,18]. In [8], the decomposition mechanism of AlMgB 14 in the SPS process at temperatures above 1400 • C was investigated.…”
Section: Shs Powdersmentioning
confidence: 99%
“…The structure was formed in the course of in situ synthesis supported by exothermic reactions between the initial mixture components. It should be noted that the SH synthesis process is supported by the heat produced by these reactions, thus making it possible to obtain powder materials without external energy input [ 14 , 15 , 16 , 17 ]. One of the main disadvantages of the SHS method is high porosity of synthesized materials [ 18 ].…”
Section: Introductionmentioning
confidence: 99%