Abstract: Nanofibre mats of poly(vinyl alcohol) (PVA), waterborne polyurethane (WBPU) and nanometre silver (Ag) colloids have been fabricated by an electrospinning method in aqueous solutions. Since PVA is a water soluble and biocompatible polymer, it is one of the best materials for preparation of electrospun antibacterial nanofibre mats. WBPU was used as a filler to enhance the properties of homopolymer nanofibre. Transmission electron microscopy analyses showed a uniform distribution of silver in the fibres. In anti-… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
8
0

Year Published

2014
2014
2024
2024

Publication Types

Select...
7
2

Relationship

1
8

Authors

Journals

citations
Cited by 11 publications
(9 citation statements)
references
References 39 publications
0
8
0
Order By: Relevance
“…PU/Ag nanofiber fabrics containing 0.01, 0.1, and 1 wt % AgNPs also have smooth surfaces. 29 The PU/Ag(5%) was linked through fusion-bonding.
Figure 4.SEM image of (a) pristine PU, (b) PU/Ag (0.01 wt%), (c) PU/Ag (0.1 wt%), (d) PU/Ag (1 wt%), and (e) PU/Ag (5 wt%).
…”
Section: Resultsmentioning
confidence: 99%
“…PU/Ag nanofiber fabrics containing 0.01, 0.1, and 1 wt % AgNPs also have smooth surfaces. 29 The PU/Ag(5%) was linked through fusion-bonding.
Figure 4.SEM image of (a) pristine PU, (b) PU/Ag (0.01 wt%), (c) PU/Ag (0.1 wt%), (d) PU/Ag (1 wt%), and (e) PU/Ag (5 wt%).
…”
Section: Resultsmentioning
confidence: 99%
“…44 Moreover, the XRD peaks for the AgNPs are found at 38.2° and 44.6° of 2θ, which are indexed to the (111) and (200) planes with cubic symmetry, respectively. 45 This indicates that the as-prepared AgNPs crystals were stabilized in these samples due to the existence of PVA molecules, even for the ultrasmall ones. However, the peaks of the silver nanocrystals from the PVA-Ag sample, which contains the lowest content of AgNPs, can barely been detected due to the resolution limit of XRD analysis.…”
Section: International Journal Of Nanomedicine Downloaded From Httpsmentioning
confidence: 90%
“…14 Recently, a series of monodispersed AgNPs with 25,35,45, 60 and 70 nm sizes was reported by using poly(vinyl pyrrolidone) (PVP) as the surfactant. 15 Also AgNPs can be incorporated within biodegradable poly(lactic acid) 16 or deposited onto modified titanium surfaces 17 as an antibacterial scaffold for tissue engineering and medical applications.…”
Section: Introductionmentioning
confidence: 99%
“…The first incorporation method of Ag NPs into the polymeric solution is the simplest, and it has been widely used. Recent works have reported the development of antibacterial ENFs thanks to this method, using polymers such as PVA [ 120 ], PVP [ 121 ], or poly(vinylidene fluoride) (PVDF) [ 122 ].…”
Section: Reviewmentioning
confidence: 99%