Electrodeposition of Au nanoparticles on poly(diallyldimethylammonium chloride) functionalized reduced graphene oxide sheets for voltammetric determination of nicotine in tobacco products and anti-smoking pharmaceuticals

Abstract: The principal objective of this study was to develop a sensitive and selective electrochemical sensor for nicotine detection based on a novel PDDA-RGO/Au nanocomposite.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2016
2016
2022
2022

Publication Types

Select...
5
2

Relationship

0
7

Authors

Journals

citations
Cited by 14 publications
(2 citation statements)
references
References 56 publications
0
2
0
Order By: Relevance
“…After rinsing that modified electrode above, 20 μL of 1 μM probe RNA was introduced for 2 h incubation at 37 °C, and then it was rinsed to obtain the PEC biosensor. Synthesis of depositing Au NPs directly on the surface of ZnSe-COOH NFs was according to the reported method . The other related experimental procedures for the modification of the electrode were as same as the above process.…”
Section: Methodsmentioning
confidence: 99%
“…After rinsing that modified electrode above, 20 μL of 1 μM probe RNA was introduced for 2 h incubation at 37 °C, and then it was rinsed to obtain the PEC biosensor. Synthesis of depositing Au NPs directly on the surface of ZnSe-COOH NFs was according to the reported method . The other related experimental procedures for the modification of the electrode were as same as the above process.…”
Section: Methodsmentioning
confidence: 99%
“…Figure 4 shows the site of absorption bands of functional groups in GO. The ex of broad stretching peaks at 3409 cm −1 , 2925 cm −1 , and 2857 cm −1 are stretching asym and symmetric a hydroxyl (O-H) and C-H groups of GO matrix [38][39][40]45], respe Moreover, the C=O stretching peak of the carboxylic (COOH) group at 1724 cm −1 , s ing band at 1626 cm −1 of aromatic C=C matrix of GO, and phenolic C-O mation,stretching, and epoxy C-O-C stretching were recognized at 1387, 1224 an cm −1 , respectively [38][39][40]46,47]. FT-IR spectroscopy is vital for describing functional moieties involved on GO's surface.…”
Section: Characterization Of the Synthesized Gomentioning
confidence: 99%