Electrode modified with nanoporous silicate submicrometre particles with appended ionic liquid

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
8
0

Year Published

2010
2010
2018
2018

Publication Types

Select...
7

Relationship

3
4

Authors

Journals

citations
Cited by 10 publications
(8 citation statements)
references
References 33 publications
0
8
0
Order By: Relevance
“…Typically, organic polymer microparticles require other polymer matrix (for example Nafion [313]) matrix for stable immobilization. This is also possible in the absence polymeric scaffold film as shown for imidazolium-appended silicate submicroparticles deposited on ITO surface by dropping methanol suspension [314]. Due to their imidazolium functional groups, this electrode acts as a reversible sponge for electroactive anions.…”
Section: Electrodes Modified With Appended Ionic Liquidsmentioning
confidence: 97%
See 1 more Smart Citation
“…Typically, organic polymer microparticles require other polymer matrix (for example Nafion [313]) matrix for stable immobilization. This is also possible in the absence polymeric scaffold film as shown for imidazolium-appended silicate submicroparticles deposited on ITO surface by dropping methanol suspension [314]. Due to their imidazolium functional groups, this electrode acts as a reversible sponge for electroactive anions.…”
Section: Electrodes Modified With Appended Ionic Liquidsmentioning
confidence: 97%
“…Immobilization of IL-appended organic polymer [313] or solgel-processed silicate [314] particles represent alternative way of IL coupling to the electrode surface. Typically, organic polymer microparticles require other polymer matrix (for example Nafion [313]) matrix for stable immobilization.…”
Section: Electrodes Modified With Appended Ionic Liquidsmentioning
confidence: 99%
“…The electroactive part of the sensor was prepared from commercially available CNPs and synthesized TMA particles. The latter were prepared using the modified Stöber method as earlier described . Briefly, 537 μl of TMOS and 105.5 μl of TMA solution in 9 ml of methanol was mixed with a solution of 0.5 g CTAB and 3 ml of NH 3 (aq) in 10 ml of water.…”
Section: Methodsmentioning
confidence: 90%
“…Ionic liquid precursor 1-methyl-3-(3-trimethoxysilylpropyl)imidazolium bis(trifluoromethyl sulfonyl)imide was synthesized as described earlier [24]. It was used together with TMOS for cationic silicate submicrometre particles preparation [20]. Their suspension was prepared by mixing 5 mg of particles with 1 ml of methanol and the mixture was sonicated for 30 min.…”
Section: Chemicals and Materialsmentioning
confidence: 99%
“…The first component was obtained from ionic liquid precursor. These particles adsorb on indium tin oxide (ITO) electrode from methanol and act as sponge for redox active anions in aqueous solution [20]. CNPs were earlier used for LbL film electrode preparation with the use of cationic polymer as a linker [12,[21][22][23]].…”
Section: Introductionmentioning
confidence: 99%